MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Essentium High Performance PLA Additive Manufacturing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Essentium PLA has been specifically designed for use in additive manufacturing. Superior tensile strength, modulus and impact resistance in comparison to standard PLA. High heat deflection temperature from excellent heat resistance and faster crystallization rates. Prints with great detail at high speeds, provides less warping, good bed adhesion.

Definitions of axes used in property data table: XY is the print direction. ZX is the build direction. YX is the third orthogonal axis.

Information provided by Essentium Materials, LLC.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³Molded; ISO 1183
Melt Flow 7.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
7.0 - 9.0 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 43.0 MPa6240 psiZX; ASTM D 638
 51.0 MPa7400 psiYX; ASTM D 638
 61.0 MPa8850 psiXY; ASTM D 638
 66.0 MPa9570 psiMolded; ASTM D 638
Tensile Modulus 2.824 GPa409.6 ksiZX; ASTM D 638
 3.167 GPa459.3 ksiYX; ASTM D 638
 3.387 GPa491.2 ksiXY; ASTM D 638
 3.538 GPa513.1 ksiMolded; ASTM D 638
Flexural Strength 64.0 MPa9280 psiYX; ASTM D 638
 73.0 MPa10600 psiZX; ASTM D 638
 105 MPa15200 psiXY; ASTM D 638
 126 MPa18300 psiMolded; ASTM D 638
Flexural Modulus 2.307 GPa334.6 ksiYX; ASTM D 790
 2.696 GPa391.0 ksiZX; ASTM D 790
 3.167 GPa459.3 ksiXY; ASTM D 790
 4.357 GPa631.9 ksiMolded; ASTM D 790
Izod Impact, Notched 0.310 J/cm0.581 ft-lb/inXY; ASTM D 256
 0.320 J/cm0.599 ft-lb/inMolded; ASTM D 256
 0.400 J/cm0.749 ft-lb/inYX; ASTM D 256
 0.400 J/cm0.749 ft-lb/inZX; ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 - 180 °C329 - 356 °FASTM D 3418
Maximum Service Temperature, Air 70.0 °C158 °FHeat deflection temperature, load unknown; ASTM D 648
Glass Transition Temp, Tg 55.0 - 60.0 °C131 - 140 °FASTM D 3418
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 240 °C374 - 464 °FExtrusion Temperature
Nozzle Temperature 235 °C455 °F
 
Descriptive Properties
Bed Temperature, °C23-60
Enclosure Temperature, °CRoom Temperature
Print SettingsInfill.: 100%; 30 mm/s, layer height: 0.3mm, extrusion multiplier: 1.0, nozzle diameter: 1.0 mm
Print Speed, mm/s30-70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
Clariant Polylactic Acid Black 3D Printer Filament
Clariant Polylactic Acid Natural Color 3D Printer Filament
Clariant Polylactic Acid White 3D Printer Filament
Clariant Polylactic Acid Red 3D Printer Filament

PESSEN905 / 220993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.