HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where applications which require excellent environmental stress crack resistance (ESCR). This material meets the Food and Drug Administration requirements of 21CFR 177.1520. |
Excellent environmental stress crack resistance (ESCR) |