MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos J50-200-178 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Narrow molecular weight distribution
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D4883
ESCR 10% Igepal® 12 hour12 hourCondition B, ASTM D1693
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 26.9 MPa3900 psi2 in/min.; ASTM D638
Elongation at Break >= 800 %>= 800 %2 in/min.; ASTM D638
Flexural Modulus 1.276 GPa185.1 ksiTangent-Method 1; ASTM D790
Izod Impact, Notched 1.23 J/cm2.30 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C171 °FASTM D648
Vicat Softening Point 131 °C268 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D 746
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ProcessInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos K54-05 HDPE
Ineos B53-35H-100 HDPE
Ineos CP52-35 HDPE
Ineos K50-10-136 HDPE
Ineos J50-2000-119 HDPE

PSOLKM009 / 68240

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.