MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos K50-10-136 HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Ineos K50-10-136 is a high molecular weight, high density polyethylene copolymer. This product was developed for blowmolding automotive fuel tanks and other large parts, where the finished product demands outstanding physical performance. K50-10-136 combines excellent processability and environmental stress crack resistance (ESCR) with superior impact and other well-balanced end use properties.

Key Words: Excellent processability and ESCR with superior impact
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D4883
Environmental Stress Crack Resistance >= 500 hour>= 500 hourASTM D1693A
High Load Melt Index 9.0 g/10 min9.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength, Yield 25.51 MPa3700 psi2 in/min (50 mm/min); ASTM D638
Elongation at Break 800 %800 %2 in/min (50 mm/min); ASTM D638
Flexural Modulus 1.138 GPa165.1 ksiTangent-Method 1; ASTM D790
Izod Impact, Notched 4.00 J/cm7.49 ft-lb/inPartial break; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C162 °FASTM D648
Vicat Softening Point 132 °C270 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746
 
Descriptive Properties
processBlow Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H01H-00 Polypropylene Homopolymer
Ineos A60-70-162 HDPE
Ineos K54-05 HDPE
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 1403-2 BK ND3007 PA66 (Conditioned)

PSOLJO / 68194

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.