MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Garlock 8316 EPDM Sheet Rubber Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Ethylene propylene diene monomer (EPDM)
FDA-approved. Recommended for service against aqueous foods.

Information provided by Garlock Rubber Technologies

Key Words: ethylene propylene diene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55 - 65ASTM D 2240
Tensile Strength 1000 psiASTM F152
Elongation at Break >= 300 %ASTM D 395
Compression Set <= 25 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D 395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
@Pressure 1.72 MPa
Minimum Service Temperature, Air -40.0 °F
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Garlock 563 EPDM Sheet Rubber
Garlock 8314 EPDM Sheet Rubber Gasketing
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert
Garlock STRESS SAVER® 370 EPDM/PTFE Gasketing
Colorite Polymers 6588 Non-Phthalate 88 Series Vinyl Compound

PGARL962B / 157535

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.