MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock 8314 EPDM Sheet Rubber Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Ethylene Propylene Diene Monomer (EPDM)
Resists weathering, ozone, and UV exposure.

Information provided by Garlock Rubber Technologies

Key Words: ethylene propylene diene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6555 - 65ASTM D 2240
Tensile Strength 6.89 MPa1000 psiASTM F152
Elongation at Break >= 300 %>= 300 %ASTM D 395
Compression Set <= 25 %
@Temperature 70.0 °C,
Time 79200 sec
<= 25 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D 395
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 0.157 kV/mm
@Thickness 3.17 mm
4.00 kV/in
@Thickness 0.125 in
Unconditioned; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C
@Pressure 1.72 MPa
300 °F
@Pressure 250 psi
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Garlock 563 EPDM Sheet Rubber
Ethylene Propylene Rubber (EPM, EPDM)
Garlock 8316 EPDM Sheet Rubber Gasketing
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert
Garlock 567 EPDM Sheet Rubber

PGARL962A / 157529

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.