MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock STRESS SAVER® 370 EPDM/PTFE Gasketing
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Molded EPDM elastomer with PTFE encapsulation. Designed for the microchip industry.
  • Raised, molded-in sealing rings seal with 75% less surface area for high performance in non-metallic flanges
  • High purity, contaminant-free EPDM is ideal for pure service-electronics, pharmaceutical and food industries
  • Proprietary process bonds PTFE to elastomer, won't delaminate or leach
Media: Acids, caustics, gases, water, hydrocarbons

Information provided by Garlock Rubber Technologies

Key Words: ethylene propylene diene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60 - 7060 - 70
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C
@Pressure 1.72 MPa
300 °F
@Pressure 250 psi
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
ColorSky Blue/Off-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Garlock 563 EPDM Sheet Rubber
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert
Garlock 567 EPDM Sheet Rubber
Garlock 8316 EPDM Sheet Rubber Gasketing
Colorite Polymers 6588 Non-Phthalate 88 Series Vinyl Compound

PGARL828 / 157511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.