MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2170 MPa
@Temperature 25.0 °C
0°, Dry
Elongation at Yield 1.4 %0°, Dry
Tensile Modulus 145 GPa0°, Dry
Flexural Yield Strength 1700 MPa
@Temperature 25.0 °C
0°, Dry
Flexural Modulus 123 GPa
@Temperature 25.0 °C
0°, Dry
Compressive Yield Strength 262 MPa
@Temperature 82.0 °C
Open hole compression, Wet
 303 MPa
@Temperature 25.0 °C
After 1500 in-inlb/in impact, Dry
 303 MPa
@Temperature 25.0 °C
Open hole compression, Dry
 1170 MPa
@Temperature 82.0 °C
0°, Wet
 1240 MPa
@Temperature 121 °C
0°, Dry
 1410 MPa
@Temperature 82.0 °C
0°, Dry
 1590 MPa
@Temperature 25.0 °C
0°, Dry
Compressive Modulus 123 GPa
@Temperature 82.0 °C
0°, Wet
 127 GPa
@Temperature 121 °C
0°, Dry
 129 GPa
@Temperature 104 °C
0°, Wet
 138 GPa
@Temperature 25.0 °C
0°, Dry
Shear Strength 50.3 MPa
@Temperature 121 °C
Short Beam, Wet
 65.5 MPa
@Temperature 121 °C
Short Beam, Dry
 82.7 MPa
@Temperature 82.0 °C
Short Beam, Wet
 84.8 MPa
@Temperature 82.0 °C
Short Beam, Dry
 107 MPa
@Temperature 25.0 °C
Short Beam, Dry
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °FEpoxy Matrix Limit

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Hexcel® HexPly® F650 Bismaleimide Resin with Fiberglass 7781 fabric reinforcement
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Hexcel® HexPly® 8551-7 Epoxy Matrix

PHEXC047 / 98517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.