Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength, Yield | 10.9 MPa @Temperature 25.0 °C | 1580 psi @Temperature 77.0 °F |
| 57.9 MPa @Temperature 25.0 °C | 8400 psi @Temperature 77.0 °F |
| 75.8 MPa @Temperature 25.0 °C | 11000 psi @Temperature 77.0 °F |
| 931 MPa @Temperature 25.0 °C | 135000 psi @Temperature 77.0 °F |
| 2760 MPa @Temperature 25.0 °C | 400000 psi @Temperature 77.0 °F |
Elongation at Yield | 1.0 % @Temperature 25.0 °C | 1.0 % @Temperature 77.0 °F |
| 1.64 % @Temperature 25.0 °C | 1.64 % @Temperature 77.0 °F |
Tensile Modulus | 8.34 GPa @Temperature 25.0 °C | 1210 ksi @Temperature 77.0 °F |
| 159 GPa @Temperature 25.0 °C | 23100 ksi @Temperature 77.0 °F |
Compressive Yield Strength | 228 MPa @Temperature 25.0 °C | 33100 psi @Temperature 77.0 °F |
| 248 MPa @Temperature 104 °C | 36000 psi @Temperature 219 °F |
| 255 MPa @Temperature 82.0 °C | 37000 psi @Temperature 180 °F |
| 290 MPa @Temperature 25.0 °C | 42100 psi @Temperature 77.0 °F |
| 303 MPa @Temperature 25.0 °C | 43900 psi @Temperature 77.0 °F |
| 324 MPa @Temperature 25.0 °C | 47000 psi @Temperature 77.0 °F |
| 345 MPa @Temperature 25.0 °C | 50000 psi @Temperature 77.0 °F |
| 462 MPa @Temperature 25.0 °C | 67000 psi @Temperature 77.0 °F |
| 586 MPa @Temperature 25.0 °C | 85000 psi @Temperature 77.0 °F |
| 1100 MPa @Temperature 82.0 °C | 160000 psi @Temperature 180 °F |
| 1280 MPa @Temperature 121 °C | 186000 psi @Temperature 250 °F |
| 1380 MPa @Temperature 82.0 °C | 200000 psi @Temperature 180 °F |
| 1620 MPa @Temperature 25.0 °C | 235000 psi @Temperature 77.0 °F |
Compressive Modulus | 143 GPa @Temperature 82.0 °C | 20700 ksi @Temperature 180 °F |
| 145 GPa @Temperature 82.0 °C | 21000 ksi @Temperature 180 °F |
| 148 GPa @Temperature 25.0 °C | 21500 ksi @Temperature 77.0 °F |
| 150 GPa @Temperature 104 °C | 21800 ksi @Temperature 219 °F |
| 152 GPa @Temperature 121 °C | 22000 ksi @Temperature 250 °F |
Shear Modulus | 5.86 GPa @Temperature 25.0 °C | 850 ksi @Temperature 77.0 °F |
Shear Strength | 40.0 MPa @Temperature 129 °C | 5800 psi @Temperature 264 °F |
| 56.5 MPa @Temperature 121 °C | 8190 psi @Temperature 250 °F |
| 68.9 MPa @Temperature 121 °C | 9990 psi @Temperature 250 °F |
| 68.9 MPa @Temperature 82.0 °C | 9990 psi @Temperature 180 °F |
| 79.3 MPa @Temperature 82.0 °C | 11500 psi @Temperature 180 °F |
| 100 MPa @Temperature 25.0 °C | 14500 psi @Temperature 77.0 °F |
| 117 MPa @Temperature 25.0 °C | 17000 psi @Temperature 77.0 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Maximum Service Temperature, Air | 93.3 °C | 200 °F |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.