MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  91.7 MPa
@Temperature 104 °C
13300 psi
@Temperature 220 °F
90°, Dry
 111 MPa
@Temperature 25.0 °C
16100 psi
@Temperature 77.0 °F
90°, Dry
 174 MPa
@Temperature -55.0 °C
25300 psi
@Temperature -67.0 °F
90°, Dry
 428 MPa
@Temperature 25.0 °C
62100 psi
@Temperature 77.0 °F
Open Hole Tensile, Dry
 2540 MPa
@Temperature 104 °C
368000 psi
@Temperature 220 °F
0°, Dry
 2570 MPa
@Temperature -55.0 °C
373000 psi
@Temperature -67.0 °F
0°, Dry
 2720 MPa
@Temperature 25.0 °C
395000 psi
@Temperature 77.0 °F
0°, Dry
Tensile Modulus  10.3 GPa
@Temperature 220 °C
1500 ksi
@Temperature 428 °F
90°, Dry
 11.7 GPa
@Temperature 77.0 °C
1700 ksi
@Temperature 171 °F
90°, Dry
 19.3 GPa
@Temperature -67.0 °C
2800 ksi
@Temperature -88.6 °F
90°, Dry
 163 GPa
@Temperature -67.0 °C
23700 ksi
@Temperature -88.6 °F
0°, Dry
 163 GPa
@Temperature 220 °C
23700 ksi
@Temperature 428 °F
0°, Dry
 164 GPa
@Temperature 77.0 °C
23800 ksi
@Temperature 171 °F
0°, Dry
Flexural Yield Strength 1860 MPa
@Temperature 25.0 °C
270000 psi
@Temperature 77.0 °F
0°, Dry
Flexural Modulus 15.2 GPa
@Temperature 25.0 °C
2200 ksi
@Temperature 77.0 °F
0°, Dry
Compressive Yield Strength  170 MPa
@Temperature 82.2 °C
24600 psi
@Temperature 180 °F
0°, Wet, Fill Compression
 214 MPa
@Temperature 25.0 °C
31000 psi
@Temperature 77.0 °F
Compression After Impact, Dry
 226 MPa
@Temperature 104 °C
32800 psi
@Temperature 220 °F
0°, Dry, Fill Compression
 234 MPa
@Temperature 25.0 °C
34000 psi
@Temperature 77.0 °F
After 1500 in-in-lb/in impact, Dry
 236 MPa
@Temperature 25.0 °C
34200 psi
@Temperature 77.0 °F
0°, Wet, Fill Compression
 305 MPa
@Temperature 25.0 °C
44200 psi
@Temperature 77.0 °F
0°, Dry, Fill Compression
 336 MPa
@Temperature 25.6 °C
48800 psi
@Temperature 78.0 °F
Open Hole Compression, Dry
 1480 MPa
@Temperature 90.6 °C
215000 psi
@Temperature 195 °F
0°, Dry
 1690 MPa
@Temperature 25.0 °C
245000 psi
@Temperature 77.0 °F
0°, Dry
Compressive Modulus  150 GPa
@Temperature 25.0 °C
21700 ksi
@Temperature 77.0 °F
0°, Dry
 162 GPa
@Temperature 90.6 °C
23500 ksi
@Temperature 195 °F
0°, Dry
Shear Strength  80.0 MPa
@Temperature 82.2 °C
11600 psi
@Temperature 180 °F
0° Short Beam, Wet
 93.8 MPa
@Temperature 104 °C
13600 psi
@Temperature 220 °F
0° Short Beam, Dry
 106 MPa
@Temperature 104 °C
15400 psi
@Temperature 220 °F
+/- 45° In-Plane, Dry
 115 MPa
@Temperature 25.0 °C
16700 psi
@Temperature 77.0 °F
0° Short Beam, Wet
 120 MPa
@Temperature 25.0 °C
17400 psi
@Temperature 77.0 °F
+/- 45° In-Plane, Dry
 137 MPa
@Temperature 25.0 °C
19900 psi
@Temperature 77.0 °F
0° Short Beam, Dry
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FEpoxy Matrix Limit

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 8552 Epoxy Matrix
Solvay CYCOM® 977-6 Epoxy Laminate with IM7 Unidirectional Tape
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Hexcel® HexTow® IM7 Carbon Fiber - Epoxy Composite

PHEXC053 / 98523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.