MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 13.3 ksi
@Temperature 104 °C
90°, Dry
 16.1 ksi
@Temperature 25.0 °C
90°, Dry
 25.3 ksi
@Temperature -55.0 °C
90°, Dry
 62.1 ksi
@Temperature 25.0 °C
Open Hole Tensile, Dry
 368 ksi
@Temperature 104 °C
0°, Dry
 373 ksi
@Temperature -55.0 °C
0°, Dry
 395 ksi
@Temperature 25.0 °C
0°, Dry
Tensile Modulus 1500 ksi
@Temperature 220 °C
90°, Dry
 1700 ksi
@Temperature 77.0 °C
90°, Dry
 2800 ksi
@Temperature -67.0 °C
90°, Dry
 23700 ksi
@Temperature -67.0 °C
0°, Dry
 23700 ksi
@Temperature 220 °C
0°, Dry
 23800 ksi
@Temperature 77.0 °C
0°, Dry
Flexural Yield Strength 270 ksi
@Temperature 25.0 °C
0°, Dry
Flexural Modulus 2200 ksi
@Temperature 25.0 °C
0°, Dry
Compressive Yield Strength 24.6 ksi
@Temperature 82.2 °C
0°, Wet, Fill Compression
 31.0 ksi
@Temperature 25.0 °C
Compression After Impact, Dry
 32.8 ksi
@Temperature 104 °C
0°, Dry, Fill Compression
 34.0 ksi
@Temperature 25.0 °C
After 1500 in-in-lb/in impact, Dry
 34.2 ksi
@Temperature 25.0 °C
0°, Wet, Fill Compression
 44.2 ksi
@Temperature 25.0 °C
0°, Dry, Fill Compression
 48.8 ksi
@Temperature 25.6 °C
Open Hole Compression, Dry
 215 ksi
@Temperature 90.6 °C
0°, Dry
 245 ksi
@Temperature 25.0 °C
0°, Dry
Compressive Modulus 21700 ksi
@Temperature 25.0 °C
0°, Dry
 23500 ksi
@Temperature 90.6 °C
0°, Dry
Shear Strength 11.6 ksi
@Temperature 82.2 °C
0° Short Beam, Wet
 13.6 ksi
@Temperature 104 °C
0° Short Beam, Dry
 15.4 ksi
@Temperature 104 °C
+/- 45° In-Plane, Dry
 16.7 ksi
@Temperature 25.0 °C
0° Short Beam, Wet
 17.4 ksi
@Temperature 25.0 °C
+/- 45° In-Plane, Dry
 19.9 ksi
@Temperature 25.0 °C
0° Short Beam, Dry
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °FEpoxy Matrix Limit

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® 8552 Epoxy Matrix
Solvay CYCOM® 977-6 Epoxy Laminate with IM7 Unidirectional Tape
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Hexcel® HexTow® IM7 Carbon Fiber - Epoxy Composite

PHEXC053 / 98523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.