MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo STYRON A-TECH™ 1210 High-Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: STYRON A-TECH™ 1210 is a newly developed, high-impact polystyrene (HIPS) reins based on patented technology, offering a unique combination of toughness, low gloss, stiffness, processability and surface smoothness.

Main Characteristics:

  • Low gloss and smooth sheet surface
  • Ease of processing
  • Excellent thermoforming behavior
  • Good blendability with General Purpose Polystyrene (GPPS)
Applications:
  • Form Fill Seal (FFS) dairy packaging
  • Medial device packaging
  • Signage sheet
  • sheet applications requiring matt and smooth surface
Complies with:
  • Europe REGULATION (EC) 10/2011
  • FDA, 21 CFR.177.1640
  • Consult the regulations for complete details

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Apparent Bulk Density 0.600 g/ccISO 60
Melt Flow 3.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 3.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure B; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22.0 MPa5 mm/min; ASTM D638
 22.0 MPaISO 527-2/5
Tensile Strength, Yield 19.5 MPa5 mm/min; ASTM D638
 19.5 MPaISO 527-2/5
Elongation at Break 65 %ASTM D638
Tensile Modulus 1750 MPa5 mm/min; ASTM D638
 1750 MPaISO 527-2/1
Flexural Strength 38.0 MPaMethod I (3 point load), 1.3 mm/min; ASTM D790
 38.0 MPaISO 178
Flexural Modulus 1950 MPaMethod I (3 point load), 1.3 mm/min; ASTM D790
 1950 MPaISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²ISO 180/4A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 98.0 °CRate B (120°C/h), Loading 1 (10N); ISO 306/A120
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo STYRON™ C-TECH High-Impact Polystyrene
Tabriz WT1235 High Impact Polystyrene
Trinseo STYRON X-TECH™ 2175 High-Impact Polystyrene
Americas Styrenics STYRON® EA6740 High Impact Polystyrene
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene

PTRINS9092 / 197565

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.