MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo STYRON X-TECH™ 2175 High-Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: STYRON X-TECH™ is an environmental stress crack resistant (ESCR) HIPS resin especially developed for thermoforming and extrusion, especially for the refrigeration industry, the production of inner liners for fridges and freezers. Based on patented Trinseo technology, this resin allows potentially 5% down gauging of the average sheet extrusion thickness for thermoforming of the inner liners, through its unique combination of ESCR, rigidity and melt strength.

Main Characteristics:

  • Allows for down-gauging
  • ESCR to food stuff and hydrocarbons
  • Ease of processing in extrusion and thermoforming
  • Excellent thermoforming behavior
  • Increased rigidity
Applications:
  • Large appliance/refrigeration liners
  • General extrusion thermoforming applications requiring ESCR
Complies with:
  • Europe REGULATION (EC) 10/2011
  • FDA, 21 CFR.177.1640
  • Consult the regulations for complete details.

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Apparent Bulk Density 0.600 g/cc0.0217 lb/in³ISO 60
Melt Flow 2.6 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.6 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  24.0 MPa
@Thickness 3.20 mm
3480 psi
@Thickness 0.126 in
5 mm/min; ASTM D638
 24.0 MPa
@Thickness 3.20 mm
3480 psi
@Thickness 0.126 in
ISO 527-2/5
Tensile Strength, Yield  16.0 MPa
@Thickness 3.20 mm
2320 psi
@Thickness 0.126 in
5 mm/min; ASTM D638
 16.0 MPa
@Thickness 3.20 mm
2320 psi
@Thickness 0.126 in
ISO 527-2/5
Elongation at Break  89 %
@Thickness 3.20 mm
89 %
@Thickness 0.126 in
5 mm/min, Injection Molded; ASTM D638
 89 %
@Thickness 3.20 mm
89 %
@Thickness 0.126 in
ISO 527-2/5
Tensile Modulus  1.70 GPa
@Thickness 3.20 mm
247 ksi
@Thickness 0.126 in
5 mm/min; ASTM D638
 1.70 GPa
@Thickness 3.20 mm
247 ksi
@Thickness 0.126 in
ISO 527-2/5
Flexural Strength  37.0 MPa
@Thickness 3.20 mm
5370 psi
@Thickness 0.126 in
Compression Molded, Method I (3 point load), 1.3 mm/min; ASTM D790
 37.0 MPa
@Thickness 3.20 mm
5370 psi
@Thickness 0.126 in
Compression Molded, 3 point load, 1.3 mm/min; ISO 178
Flexural Modulus 1.80 GPa261 ksiCompression Molded, Method I (3 point load), 1.3 mm/min; ASTM D790
 1.80 GPa261 ksiCompression Molded, 3 point load, 1.3 mm/min; ISO 178
Izod Impact, Notched  0.0640 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
0.120 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 0.0890 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
0.167 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched  0.660 J/cm²
@Temperature -30.0 °C
3.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1A
 0.910 J/cm²
@Temperature 23.0 °C
4.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C180 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C156 °FUnannealed; ISO 75-2/A
Vicat Softening Point 90.0 °C194 °FISO 306/B50
 99.0 °C210 °FISO 306/A120
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo STYRON A-TECH™ 1175 Polystyrene Resin
Trinseo STYRON™ C-TECH High-Impact Polystyrene
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene
SYNTHOS Krasten® 662E High Impact Polystyrene
Tabriz WT1235 High Impact Polystyrene

PTRINS9094 / 197567

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.