MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo STYRON™ C-TECH High-Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: STYRON™ C-TECH is a high clarity, high gloss polystyrene with excellent mechanical properties on thermoformed parts.

Main Characteristics:

  • High clarity
  • Excellent gloss
  • High heat
  • High flow
  • Easy processing
  • Excellent mechanical properties of thermoformed parts
Applications:
  • Transparent Packaging Applications: Form Fill Seal (FFS), pre-forms (DFS), Disposables and Bi-Oriented Polystyrene (BOPS).
  • Gloss cap-layer for extrusion
Complies with:
  • Europe REGULATION (EC) 10/2011
  • FDA, 21 CFR.177.1640
  • Meets Essential Req. of 94/62/EC (Packaging)

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Melt Flow 6.3 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.3 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  27.0 MPa
@Thickness 3.20 mm
3920 psi
@Thickness 0.126 in
5 mm/min; ASTM D638
 27.0 MPa
@Thickness 3.20 mm
3920 psi
@Thickness 0.126 in
ISO 527-2/5
Tensile Strength, Yield  33.0 MPa
@Thickness 3.20 mm
4790 psi
@Thickness 0.126 in
5 mm/min; ASTM D638
 33.0 MPa
@Thickness 3.20 mm
4790 psi
@Thickness 0.126 in
ISO 527-2/5
Elongation at Break  >= 20 %
@Thickness 3.20 mm
>= 20 %
@Thickness 0.126 in
5 mm/min; ASTM D638
 >= 20 %
@Thickness 3.20 mm
>= 20 %
@Thickness 0.126 in
ISO 527-2/5
Tensile Modulus  2.70 GPa
@Thickness 3.20 mm
392 ksi
@Thickness 0.126 in
5 mm/min; ASTM D638
 2.70 GPa
@Thickness 3.20 mm
392 ksi
@Thickness 0.126 in
ISO 527-2/5
Flexural Strength  62.0 MPa
@Thickness 3.20 mm
8990 psi
@Thickness 0.126 in
Method I (3 point load), 1.3 mm/min; ASTM D790
 62.0 MPa
@Thickness 3.20 mm
8990 psi
@Thickness 0.126 in
3 point load, 1.3 mm/min; ISO 178
Flexural Modulus 2.60 GPa377 ksiMethod I (3 point load), 1.3 mm/min; ASTM D790
 2.60 GPa377 ksi3 point load, 1.3 mm/min; ISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FUnannealed; ISO 75-2/A
Vicat Softening Point 100 °C212 °FISO 306/A120
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Optical PropertiesMetricEnglishComments
Gloss 60 %60 %Gardner, 60°, Thermoformed; ASTM D523
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo STYRON X-TECH™ 2175 High-Impact Polystyrene
Trinseo STYRON A-TECH™ 1175 Polystyrene Resin
Supreme Petrochem SP 263 Toughened Polystyrene
Supreme Petrochem SP 266 Toughened Polystyrene
Tabriz WT1235 High Impact Polystyrene

PTRINS9093 / 197566

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.