MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Supreme Petrochem SP 266 Toughened Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Characteristics
  • Good stiffness
  • Excellent toughness
  • High flow
  • Excellent clarity
Processing
  • Injection molding
Applications
  • Transparent hangers
  • Stationery items like pen barrels, geometric instruments
  • Medical components
Material Status: Commercial : Active

Agency Ratings: FDA 21 CFR 177.1640

Information provided by Supreme Petrochem LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
10 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.3 MPa4970 psi50 mm/min; ASTM D638
Elongation at Break 20 %20 %50 mm/min; ASTM D638
Flexural Strength 46.6 MPa
@Thickness 3.20 mm
6760 psi
@Thickness 0.126 in
ASTM D790
Flexural Modulus 1.77 GPa
@Thickness 3.20 mm
256 ksi
@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 0.150 J/cm
@Thickness 3.20 mm
0.281 ft-lb/in
@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 3.25 J/cm
@Thickness 3.20 mm
6.09 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FASTM D648
Vicat Softening Point 98.0 °C208 °F1kg load; 120°C/h; ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %
@Thickness 1.00 mm
1.0 %
@Thickness 0.0394 in
SPL test method
Transmission, Visible 88 %
@Thickness 1.00 mm
88 %
@Thickness 0.0394 in
SPL test method
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 220 °C<= 428 °F
Mold Temperature 40.0 - 50.0 °C104 - 122 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo STYRON™ C-TECH High-Impact Polystyrene
Supreme Petrochem SP 263 Toughened Polystyrene
Total PSC 1960N Crystal Polystyrene
Dow AIM® 4800 High Impact Styrenic Resin
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance

PSUP32 / 69464

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.