MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other heat cures can be used.

Advantages & Application Notes:

  • Ease of use: smooth flowing paste allows for automated dispensing, stamping, brushing, or hand applications. In some cases, the low viscosity nature of the paste allows it to be sprayed onto targets.
  • Suggested applications include: EMI and Rf shielding, ITO interconnects in LCDs, low temperature cryogenic cooling.
  • Exhibits superior adhesion to a wide variety of substrates including most metals, ceramics, glass and plastics.
  • Hybrid / Micro-electronic adhesive including die-attach and substrate attach for Rf and Microwave devices.
  • Bright and shiny silver epoxy; provides a metallic-like layer after cure.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccPart B
 3.10 g/cc3.10 g/ccPart A
Particle Size <= 45 µm<= 45 µm
Viscosity 800 - 1600 cP
@Temperature 23.0 °C
800 - 1600 cP
@Temperature 73.4 °F
100 rpm
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) 23 ppm23 ppm
Ionic Impurities - K (Potassium) 31 ppm31 ppm
Ionic Impurities - Cl (Chloride) 151 ppm151 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060
Tensile Modulus 3.58 GPa519 ksiStorage
Shear Strength 8.729 MPa1266 psiLap
 >= 11.7 MPa>= 1700 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00050 ohm-cm<= 0.00050 ohm-cm
 <= 0.00070 ohm-cm<= 0.00070 ohm-cm25°C/40-60%RH/3 Day cure
 
Thermal PropertiesMetricEnglishComments
CTE, linear 48.0 µm/m-°C26.7 µin/in-°FBelow Tg
 150 µm/m-°C83.3 µin/in-°FAbove Tg
Thermal Conductivity 1.37 W/m-K9.51 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C302 °FContinuous
 250 °C482 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 40.0 °C>= 104 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 380 °C716 °FDegradation Temperature; TGA
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 150 °C
0.250 hour
@Temperature 302 °F
Minimum Bond Line
 180 min
@Temperature 80.0 °C
3.00 hour
@Temperature 176 °F
Minimum Bond Line
 360 min
@Temperature 60.0 °C
6.00 hour
@Temperature 140 °F
Minimum Bond Line
 4320 min
@Temperature 23.0 °C
72.0 hour
@Temperature 73.4 °F
Minimum Bond Line
Pot Life 240 min240 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorClear/ColorlessPart B
 SilverPart A
ConsistencySmooth flowing paste
Ionic Impurities NH423 ppm
Mix Ratio by Weight10:1
Number of ComponentsTwo
Thixotropic Index2.1
Weight Loss0.7%200°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20E-175 Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H35-175MP Electrically Conductive, Silver Epoxy

PPOXYT014 / 141052

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.