MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.23 - 1.62 g/cc0.0444 - 0.0585 lb/in³Average value: 1.39 g/cc Grade Count:113
Filler Content 25.0 - 33.0 %25.0 - 33.0 %Average value: 30.3 % Grade Count:12
Water Absorption 0.500 - 7.00 %0.500 - 7.00 %Average value: 2.83 % Grade Count:73
Moisture Absorption at Equilibrium 1.00 - 2.50 %1.00 - 2.50 %Average value: 1.81 % Grade Count:31
 1.40 - 1.90 %
@Temperature 70.0 - 70.0 °C
1.40 - 1.90 %
@Temperature 158 - 158 °F
Average value: 1.65 % Grade Count:4
Water Absorption at Saturation 3.50 - 6.50 %3.50 - 6.50 %Average value: 4.99 % Grade Count:37
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm0.00100 - 0.0200 in/inAverage value: 0.00445 cm/cm Grade Count:78
Linear Mold Shrinkage, Transverse 0.00100 - 0.0150 cm/cm0.00100 - 0.0150 in/inAverage value: 0.00670 cm/cm Grade Count:69
Melt Flow 2.00 - 45.0 g/10 min2.00 - 45.0 g/10 minAverage value: 12.4 g/10 min Grade Count:5
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 80.0 - 270 MPa11600 - 39200 psiAverage value: 184 MPa Grade Count:46
Tensile Strength, Ultimate 45.0 - 200 MPa6530 - 29000 psiAverage value: 137 MPa Grade Count:107
Tensile Strength, Yield 70.0 - 180 MPa10200 - 26100 psiAverage value: 117 MPa Grade Count:14
Elongation at Break 1.80 - 35.0 %1.80 - 35.0 %Average value: 4.27 % Grade Count:108
Elongation at Yield 3.00 - 6.00 %3.00 - 6.00 %Average value: 4.29 % Grade Count:12
Modulus of Elasticity 1.80 - 99.4 GPa261 - 14400 ksiAverage value: 8.85 GPa Grade Count:91
Flexural Yield Strength 56.0 - 275 MPa8120 - 39900 psiAverage value: 200 MPa Grade Count:46
Flexural Modulus 3.70 - 10.5 GPa537 - 1520 ksiAverage value: 7.74 GPa Grade Count:48
Poissons Ratio 0.330 - 0.4000.330 - 0.400Average value: 0.352 Grade Count:13
Izod Impact, Notched 0.550 - 1.50 J/cm1.03 - 2.81 ft-lb/inAverage value: 1.13 J/cm Grade Count:7
Izod Impact, Notched (ISO) 4.00 - 21.0 kJ/m²1.90 - 9.99 ft-lb/in²Average value: 11.6 kJ/m² Grade Count:25
 7.20 - 11.0 kJ/m²
@Temperature -40.0 - -30.0 °C
3.43 - 5.23 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 8.48 kJ/m² Grade Count:3
Charpy Impact Unnotched 2.50 J/cm² - NB11.9 ft-lb/in² - NBAverage value: 6.44 J/cm² Grade Count:89
 2.40 J/cm² - NB
@Temperature -40.0 - -20.0 °C
11.4 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 5.14 J/cm² Grade Count:74
Charpy Impact, Notched 0.399 - 8.50 J/cm²1.90 - 40.5 ft-lb/in²Average value: 1.22 J/cm² Grade Count:96
 0.200 - 5.50 J/cm²
@Temperature -40.0 - -20.0 °C
0.952 - 26.2 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.856 J/cm² Grade Count:72
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+15 ohm-cm1.00e+9 - 1.00e+15 ohm-cmAverage value: 1.72e+14 ohm-cm Grade Count:63
Surface Resistance 1.00e+10 - 1.00e+15 ohm1.00e+10 - 1.00e+15 ohmAverage value: 1.29e+14 ohm Grade Count:43
Dielectric Constant 3.00 - 4.303.00 - 4.30Average value: 3.69 Grade Count:6
Dielectric Strength 12.0 - 60.0 kV/mm305 - 1520 kV/inAverage value: 30.2 kV/mm Grade Count:55
Dissipation Factor 0.00500 - 0.1000.00500 - 0.100Average value: 0.0206 Grade Count:11
Arc Resistance 60.0 - 120 sec60.0 - 120 secAverage value: 90.0 sec Grade Count:4
Comparative Tracking Index 175 - 650 V175 - 650 VAverage value: 534 V Grade Count:53
Hot Wire Ignition, HWI 120 sec120 secAverage value: 120 sec Grade Count:7
High Amp Arc Ignition, HAI 120 arcs120 arcsAverage value: 120 arcs Grade Count:7
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minAverage value: 115 mm/min Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 - 80.0 µm/m-°C7.78 - 44.4 µin/in-°FAverage value: 24.1 µm/m-°C Grade Count:44
 10.0 - 20.0 µm/m-°C
@Temperature 55.0 - 160 °C
5.56 - 11.1 µin/in-°F
@Temperature 131 - 320 °F
Average value: 17.2 µm/m-°C Grade Count:6
 20.0 - 20.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
11.1 - 11.1 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 17.2 µm/m-°C Grade Count:2
 20.0 - 20.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
11.1 - 11.1 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 17.2 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 45.0 - 110 µm/m-°C25.0 - 61.1 µin/in-°FAverage value: 75.0 µm/m-°C Grade Count:43
 91.0 - 130 µm/m-°C
@Temperature 55.0 - 160 °C
50.6 - 72.2 µin/in-°F
@Temperature 131 - 320 °F
Average value: 109 µm/m-°C Grade Count:6
Specific Heat Capacity 2.00 - 2.00 J/g-°C
@Temperature 280 - 280 °C
0.478 - 0.478 BTU/lb-°F
@Temperature 536 - 536 °F
Average value: 2.00 J/g-°C Grade Count:1
Thermal Conductivity 0.250 - 0.250 W/m-K
@Temperature 280 - 280 °C
1.74 - 1.74 BTU-in/hr-ft²-°F
@Temperature 536 - 536 °F
Average value: 0.250 W/m-K Grade Count:1
Melting Point 200 - 312 °C392 - 594 °FAverage value: 263 °C Grade Count:82
Maximum Service Temperature, Air 90.0 - 270 °C194 - 518 °FAverage value: 173 °C Grade Count:42
Deflection Temperature at 0.46 MPa (66 psi) 215 - 300 °C419 - 572 °FAverage value: 246 °C Grade Count:21
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 285 °C158 - 545 °FAverage value: 222 °C Grade Count:90
Deflection Temperature at 8.0 MPa 50.0 - 204 °C122 - 399 °FAverage value: 139 °C Grade Count:35
Vicat Softening Point 195 - 252 °C383 - 486 °FAverage value: 226 °C Grade Count:5
Glass Transition Temp, Tg 45.0 - 90.0 °C113 - 194 °FAverage value: 67.5 °C Grade Count:4
UL RTI, Electrical 65.0 - 160 °C149 - 320 °FAverage value: 113 °C Grade Count:11
UL RTI, Mechanical with Impact 65.0 - 105 °C149 - 221 °FAverage value: 75.9 °C Grade Count:7
UL RTI, Mechanical without Impact 65.0 - 140 °C149 - 284 °FAverage value: 88.2 °C Grade Count:7
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:65
 HB - HB
@Temperature 1.50 - 1.50 °C
HB - HB
@Temperature 34.7 - 34.7 °F
Grade Count:1
Flame Spread 80.0 mm/min3.15 in/minAverage value: 80.0 mm/min Grade Count:3
Oxygen Index 23.0 - 42.0 %23.0 - 42.0 %Average value: 34.5 % Grade Count:12
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 850 °C Grade Count:18
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 240 - 304 °C464 - 580 °FAverage value: 271 °C Grade Count:8
Melt Temperature 225 - 330 °C437 - 626 °FAverage value: 277 °C Grade Count:28
Mold Temperature 60.0 - 130 °C140 - 266 °FAverage value: 91.4 °C Grade Count:29
Drying Temperature 79.4 - 100 °C175 - 212 °FAverage value: 83.4 °C Grade Count:26
Moisture Content 0.0500 - 0.200 %0.0500 - 0.200 %Average value: 0.158 % Grade Count:20
Injection Pressure 34.5 - 138 MPa5000 - 20000 psiAverage value: 91.2 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66/6
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced

O2493 / 77994

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.