MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Nylon 6, 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.67 g/cc0.0434 - 0.0603 lb/in³Average value: 1.37 g/cc Grade Count:1119
 1.136 - 1.20 g/cc
@Temperature 220 - 270 °C
0.04104 - 0.0434 lb/in³
@Temperature 428 - 518 °F
Average value: 1.17 g/cc Grade Count:10
Filler Content 25.0 - 33.0 %25.0 - 33.0 %Average value: 29.8 % Grade Count:165
Water Absorption 0.130 - 9.00 %0.130 - 9.00 %Average value: 2.78 % Grade Count:462
Moisture Absorption at Equilibrium 0.170 - 7.10 %0.170 - 7.10 %Average value: 1.96 % Grade Count:353
 0.700 - 2.50 %
@Temperature 70.0 - 70.0 °C
0.700 - 2.50 %
@Temperature 158 - 158 °F
Average value: 1.68 % Grade Count:44
 0.550 - 1.55 %
@Temperature 70.0 - 70.0 °C
0.550 - 1.55 %
@Temperature 158 - 158 °F
Average value: 1.68 % Grade Count:1
 0.550 - 1.55 %
@Time 180000 - 1.44e+6 sec
0.550 - 1.55 %
@Time 50.0 - 400 hour
Average value: 1.68 % Grade Count:1
Water Absorption at Saturation 1.00 - 8.20 %1.00 - 8.20 %Average value: 6.18 % Grade Count:204
Additive Loading 30.0 - 33.0 %30.0 - 33.0 %Average value: 30.8 % Grade Count:4
Viscosity 2.60 - 50.0 cP2.60 - 50.0 cPAverage value: 7.04 cP Grade Count:11
 30.0 - 500 cP
@Temperature 230 - 270 °C
30.0 - 500 cP
@Temperature 446 - 518 °F
Average value: 196 cP Grade Count:3
 30.0 - 500 cP
@Shear Rate 100 - 10000 1/s
30.0 - 500 cP
@Shear Rate 100 - 10000 1/s
Average value: 196 cP Grade Count:3
Viscosity Test 125 - 150 cm³/g1.25 - 1.50 dl/gAverage value: 144 cm³/g Grade Count:14
Viscosity Number 125 - 230 cm³/g1.25 - 2.30 dl/gAverage value: 150 cm³/g Grade Count:24
Maximum Moisture Content 0.0200 - 0.2000.0200 - 0.200Average value: 0.157 Grade Count:47
Linear Mold Shrinkage 0.000500 - 0.0650 cm/cm0.000500 - 0.0650 in/inAverage value: 0.00418 cm/cm Grade Count:808
 0.00100 - 0.00300 cm/cm
@Temperature 80.0 - 80.0 °C
0.00100 - 0.00300 in/in
@Temperature 176 - 176 °F
Average value: 0.00215 cm/cm Grade Count:13
Linear Mold Shrinkage, Transverse 0.00100 - 0.0650 cm/cm0.00100 - 0.0650 in/inAverage value: 0.00768 cm/cm Grade Count:442
 0.00500 - 0.00700 cm/cm
@Temperature 80.0 - 80.0 °C
0.00500 - 0.00700 in/in
@Temperature 176 - 176 °F
Average value: 0.00638 cm/cm Grade Count:13
Melt Flow 1.00 - 101 g/10 min1.00 - 101 g/10 minAverage value: 26.2 g/10 min Grade Count:111
Spiral Flow 50.0 - 715 cm19.7 - 281 inAverage value: 102 cm Grade Count:20
Ash 25.0 - 37.0 %25.0 - 37.0 %Average value: 30.7 % Grade Count:36
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 102 - 115102 - 115Average value: 112 Grade Count:5
Hardness, Rockwell M 80.0 - 12180.0 - 121Average value: 101 Grade Count:20
Hardness, Rockwell R 82.0 - 12282.0 - 122Average value: 119 Grade Count:147
 12.0 - 12.0
@Temperature 80.0 - 80.0 °C
12.0 - 12.0
@Temperature 176 - 176 °F
Average value: 12.0 Grade Count:2
Hardness, Shore D 76.0 - 89.076.0 - 89.0Average value: 81.7 Grade Count:10
Hardness, Shore M 100100Average value: 100 Grade Count:3
Ball Indentation Hardness 70.0 - 280 MPa10200 - 40600 psiAverage value: 171 MPa Grade Count:121
Tensile Strength, Ultimate 12.2 - 1500 MPa1770 - 218000 psiAverage value: 140 MPa Grade Count:903
 20.0 - 283 MPa
@Temperature -40.0 - 150 °C
2900 - 41000 psi
@Temperature -40.0 - 302 °F
Average value: 120 MPa Grade Count:29
 125 - 150 MPa
@Temperature 70.0 - 70.0 °C
18100 - 21800 psi
@Temperature 158 - 158 °F
Average value: 120 MPa Grade Count:1
 125 - 150 MPa
@Time 180000 - 1.44e+6 sec
18100 - 21800 psi
@Time 50.0 - 400 hour
Average value: 120 MPa Grade Count:1
 30.0 - 170 MPa
@Strain 1.00 - 2.00 %
4350 - 24700 psi
@Strain 1.00 - 2.00 %
Average value: 120 MPa Grade Count:1
 30.0 - 170 MPa
@Temperature -20.0 - 150 °C
4350 - 24700 psi
@Temperature -4.00 - 302 °F
Average value: 120 MPa Grade Count:1
Tensile Strength, Yield 3.00 - 193 MPa435 - 28000 psiAverage value: 147 MPa Grade Count:239
 111 - 214 MPa
@Temperature -40.0 - 80.0 °C
16100 - 31000 psi
@Temperature -40.0 - 176 °F
Average value: 176 MPa Grade Count:2
Elongation at Break 0.800 - 180 %0.800 - 180 %Average value: 4.45 % Grade Count:1002
 2.40 - 12.0 %
@Temperature -40.0 - 150 °C
2.40 - 12.0 %
@Temperature -40.0 - 302 °F
Average value: 5.08 % Grade Count:22
Elongation at Yield 1.50 - 14.0 %1.50 - 14.0 %Average value: 3.96 % Grade Count:107
 4.60 - 7.60 %
@Temperature 60.0 - 150 °C
4.60 - 7.60 %
@Temperature 140 - 302 °F
Average value: 5.99 % Grade Count:2
Modulus of Elasticity 1.16 - 20.2 GPa168 - 2930 ksiAverage value: 7.97 GPa Grade Count:712
 2.50 - 11.6 GPa
@Temperature -40.0 - 150 °C
363 - 1680 ksi
@Temperature -40.0 - 302 °F
Average value: 5.36 GPa Grade Count:15
Flexural Yield Strength 29.0 - 800 MPa4210 - 116000 psiAverage value: 208 MPa Grade Count:782
 89.0 - 380 MPa
@Temperature -40.0 - 121 °C
12900 - 55100 psi
@Temperature -40.0 - 250 °F
Average value: 196 MPa Grade Count:11
Flexural Modulus 0.724 - 18.5 GPa105 - 2680 ksiAverage value: 7.43 GPa Grade Count:850
 2.97 - 12.5 GPa
@Temperature -40.0 - 121 °C
431 - 1810 ksi
@Temperature -40.0 - 250 °F
Average value: 5.68 GPa Grade Count:12
Flexural Strain at Break 2.00 - 11.6 %2.00 - 11.6 %Average value: 4.91 % Grade Count:101
Compressive Yield Strength 120 - 222 MPa17400 - 32200 psiAverage value: 162 MPa Grade Count:12
 70.0 - 250 MPa
@Temperature -40.0 - 80.0 °C
10200 - 36300 psi
@Temperature -40.0 - 176 °F
Average value: 156 MPa Grade Count:2
Poissons Ratio 0.340 - 0.3500.340 - 0.350Average value: 0.346 Grade Count:22
Shear Modulus 3.60 - 4.10 GPa522 - 595 ksiAverage value: 3.77 GPa Grade Count:4
Shear Strength 60.0 - 85.0 MPa8700 - 12300 psiAverage value: 76.7 MPa Grade Count:3
Izod Impact, Notched 0.370 - 3.36 J/cm0.693 - 6.30 ft-lb/inAverage value: 1.23 J/cm Grade Count:336
 0.700 - 3.84408 J/cm
@Temperature -40.0 - 121 °C
1.31 - 7.20154 ft-lb/in
@Temperature -40.0 - 250 °F
Average value: 1.18 J/cm Grade Count:8
 1.01441 - 1.33475 J/cm
@Temperature -40.0 - -40.0 °C
1.90041 - 2.50053 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 1.18 J/cm Grade Count:8
 1.01441 - 1.33475 J/cm
@Thickness 3.17 - 3.17 mm
1.90041 - 2.50053 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 1.18 J/cm Grade Count:8
Izod Impact, Unnotched 0.122 - 5340 J/cm0.229 - 10000 ft-lb/inAverage value: 10.0 J/cm Grade Count:53
Izod Impact, Notched (ISO) 1.50 - 182 kJ/m²0.714 - 86.6 ft-lb/in²Average value: 15.4 kJ/m² Grade Count:354
 3.00 - 35.0 kJ/m²
@Temperature -40.0 - -30.0 °C
1.43 - 16.7 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 10.5 kJ/m² Grade Count:127
Izod Impact, Unnotched (ISO) 2.60 kJ/m² - NB1.24 ft-lb/in² - NBAverage value: 60.2 kJ/m² Grade Count:126
 25.0 kJ/m² - NB
@Temperature -30.0 - -30.0 °C
11.9 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 58.2 kJ/m² Grade Count:76
Charpy Impact Unnotched 0.220 J/cm² - NB1.05 ft-lb/in² - NBAverage value: 7.50 J/cm² Grade Count:566
 0.700 J/cm² - NB
@Temperature -40.0 - -20.0 °C
3.33 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 6.26 J/cm² Grade Count:362
Charpy Impact, Notched 0.200 J/cm² - NB0.952 ft-lb/in² - NBAverage value: 1.48 J/cm² Grade Count:663
 0.150 - 3.50 J/cm²
@Temperature -40.0 - -20.0 °C
0.714 - 16.7 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.02 J/cm² Grade Count:359
Puncture Energy 2.00 - 14.0 J1.48 - 10.3 ft-lbAverage value: 5.42 J Grade Count:32
 1.70 - 6.00 J
@Temperature -30.0 - -30.0 °C
1.25 - 4.43 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 3.10 J Grade Count:28
Coefficient of Friction 0.150 - 0.6100.150 - 0.610Average value: 0.290 Grade Count:8
Coefficient of Friction, Static 0.190 - 0.4500.190 - 0.450Average value: 0.322 Grade Count:5
Tensile Creep Modulus, 1 hour 2400 - 92000 MPa348000 - 1.33e+7 psiAverage value: 10400 MPa Grade Count:18
Tensile Creep Modulus, 1000 hours 2000 - 6500 MPa290000 - 943000 psiAverage value: 3900 MPa Grade Count:22
Taber Abrasion, mg/1000 Cycles 0.350 - 25.00.350 - 25.0Average value: 12.4 Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 25.0 - 1.00e+18 ohm-cm25.0 - 1.00e+18 ohm-cmAverage value: 5.39e+15 ohm-cm Grade Count:431
Surface Resistance 100 - 1.00e+16 ohm100 - 1.00e+16 ohmAverage value: 1.65e+14 ohm Grade Count:261
Dielectric Constant 2.50 - 38.02.50 - 38.0Average value: 5.81 Grade Count:218
Dielectric Strength 7.87 - 80.0 kV/mm200 - 2030 kV/inAverage value: 29.2 kV/mm Grade Count:298
Dissipation Factor 0.00500 - 0.8500.00500 - 0.850Average value: 0.0875 Grade Count:187
Dielectric Loss Index 0.0220 - 0.2400.0220 - 0.240Average value: 0.125 Grade Count:10
Arc Resistance 15.0 - 180 sec15.0 - 180 secAverage value: 117 sec Grade Count:22
Comparative Tracking Index 0.000 - 600 V0.000 - 600 VAverage value: 519 V Grade Count:321
Hot Wire Ignition, HWI 15.0 - 60.0 sec15.0 - 60.0 secAverage value: 36.0 sec Grade Count:3
High Amp Arc Ignition, HAI 120 arcs120 arcsAverage value: 120 arcs Grade Count:3
High Voltage Arc-Tracking Rate, HVTR 25.4 - 150 mm/min1.00 - 5.91 in/minAverage value: 63.5 mm/min Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.50 - 82.0 µm/m-°C1.39 - 45.6 µin/in-°FAverage value: 26.4 µm/m-°C Grade Count:285
 6.00 - 14.0 µm/m-°C
@Temperature 55.0 - 160 °C
3.33 - 7.78 µin/in-°F
@Temperature 131 - 320 °F
Average value: 19.3 µm/m-°C Grade Count:4
 20.0 - 31.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
11.1 - 17.2 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 19.3 µm/m-°C Grade Count:7
 20.0 - 31.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
11.1 - 17.2 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 19.3 µm/m-°C Grade Count:7
CTE, linear, Transverse to Flow 23.0 - 150 µm/m-°C12.8 - 83.3 µin/in-°FAverage value: 81.1 µm/m-°C Grade Count:170
 110 - 130 µm/m-°C
@Temperature 55.0 - 160 °C
61.1 - 72.2 µin/in-°F
@Temperature 131 - 320 °F
Average value: 120 µm/m-°C Grade Count:4
Specific Heat Capacity 0.350 - 2.43 J/g-°C0.0837 - 0.582 BTU/lb-°FAverage value: 1.57 J/g-°C Grade Count:25
 2.20 - 2.28 J/g-°C
@Temperature 270 - 270 °C
0.526 - 0.545 BTU/lb-°F
@Temperature 518 - 518 °F
Average value: 2.24 J/g-°C Grade Count:2
Thermal Conductivity 0.200 - 1.64 W/m-K1.39 - 11.4 BTU-in/hr-ft²-°FAverage value: 0.360 W/m-K Grade Count:41
 0.230 - 0.260 W/m-K
@Temperature 270 - 270 °C
1.60 - 1.80 BTU-in/hr-ft²-°F
@Temperature 518 - 518 °F
Average value: 0.245 W/m-K Grade Count:2
Melting Point 178 - 325 °C352 - 617 °FAverage value: 224 °C Grade Count:661
Crystallization Temperature 167 - 190 °C333 - 374 °FAverage value: 182 °C Grade Count:3
Maximum Service Temperature, Air 65.0 - 288 °C149 - 550 °FAverage value: 155 °C Grade Count:123
Deflection Temperature at 0.46 MPa (66 psi) 110 - 305 °C230 - 581 °FAverage value: 215 °C Grade Count:458
Deflection Temperature at 1.8 MPa (264 psi) 65.0 - 290 °C149 - 554 °FAverage value: 204 °C Grade Count:819
Deflection Temperature at 8.0 MPa 60.0 - 213 °C140 - 415 °FAverage value: 128 °C Grade Count:56
Vicat Softening Point 145 - 313 °C293 - 595 °FAverage value: 209 °C Grade Count:208
Heat Distortion Temperature 215 - 255 °C419 - 491 °FAverage value: 230 °C Grade Count:3
Minimum Service Temperature, Air -60.0 - -20.0 °C-76.0 - -4.00 °FAverage value: -46.7 °C Grade Count:3
Glass Transition Temp, Tg 5.00 - 67.0 °C41.0 - 153 °FAverage value: 39.1 °C Grade Count:12
Decomposition Temperature 300 - 350 °C572 - 662 °FAverage value: 321 °C Grade Count:20
UL RTI, Electrical 65.0 - 140 °C149 - 284 °FAverage value: 117 °C Grade Count:36
UL RTI, Mechanical with Impact 65.0 - 125 °C149 - 257 °FAverage value: 103 °C Grade Count:36
UL RTI, Mechanical without Impact 65.0 - 150 °C149 - 302 °FAverage value: 116 °C Grade Count:35
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:582
Flame Spread 0.000 - 102 mm/min0.000 - 4.02 in/minAverage value: 31.7 mm/min Grade Count:19
Oxygen Index 21.0 - 39.8 %21.0 - 39.8 %Average value: 25.4 % Grade Count:58
Glow Wire Test 500 - 960 °C932 - 1760 °FAverage value: 771 °C Grade Count:163
Ignition Temperature 400 - 470 °C752 - 878 °FAverage value: 423 °C Grade Count:18
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 300 °C158 - 572 °FAverage value: 221 °C Grade Count:92
Nozzle Temperature 55.0 - 295 °C131 - 563 °FAverage value: 258 °C Grade Count:97
Melt Temperature 210 - 350 °C410 - 662 °FAverage value: 266 °C Grade Count:530
Mold Temperature 21.1 - 121 °C70.0 - 250 °FAverage value: 83.9 °C Grade Count:553
Drying Temperature 26.7 - 180 °C80.0 - 356 °FAverage value: 84.0 °C Grade Count:420
Moisture Content 0.00150 - 1.12 %0.00150 - 1.12 %Average value: 0.144 % Grade Count:227
Dew Point -40.0 - -17.8 °C-40.0 - 0.000 °FAverage value: -21.5 °C Grade Count:12
Injection Pressure 3.45 - 172 MPa500 - 25000 psiAverage value: 73.7 MPa Grade Count:79
Vent Depth 0.00127 - 0.00762 cm0.000500 - 0.00300 inAverage value: 0.00238 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 6, 20% Glass Fiber Filled
Overview of materials for Nylon 6, 10% Glass Fiber Filled
Overview of materials for Nylon 6, 50% Glass Fiber Filled

O2413 / 77973

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.