MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos TUB 172 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: TUB 172 is a yellow medium density polyethylene copolymer designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stress life and slow crack growth resistance. TUB 172 is the North American equivalent to ELTEX® TUB 172 Yellow produced in Europe. This material is certified to CSA Standard B137.4-05 and is recognized by the Plastics Pipe Institute as having a PE 2708 (formerly PE 2406) and PE 80 rating.

Key Words: Yellow BiModal Gas Pipe Grade
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³Natural; ASTM D4883
 0.940 g/cc0.0340 lb/in³Yellow; ASTM D4883
Oxidative Induction Time (OIT) >= 20 min>= 20 minASTM D3895
Melt Flow  0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 0.85 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.85 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 500 hour>= 500 hourNotched Tensile; ASTM F1473
Hardness, Shore D 6464ASTM D2240
Tensile Strength at Break 31.0 MPa4500 psi2 in/min; ASTM D638
Tensile Strength, Yield 19.3 MPa2800 psi2 in/min; ASTM D638
Elongation at Break >= 800 %>= 800 %2 in/min; ASTM D638
Flexural Modulus 0.689 GPa
@Strain 2 %
100 ksi
@Strain 2 %
Secant - Method 1; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 120 °C248 °FASTM D1525
Brittleness Temperature <= -118 °C<= -180 °FASTM D746
Decomposition Temperature >= 220 °C>= 428 °FThermal Stability; ASTM D2513/D3350
 
Descriptive Properties
Cell Classification234370E
processPipe Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos TUB 121 HDPE
Ineos K38-20-160 Polyethylene Copolymer
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade
Ineos K38-20-188 HDPE
Ineos TUB 121N HDPE

PSOLKM015 / 89054

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.