MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos TUB 121 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. It has NSF Standard 14 certification and complies with ANSI/NSF Standard 61 health effects requirements. TUB 121 is recognized by the Plastic Pipe Institute as having a pipe material designation code of PE 4710 and PE 100.

Key Words: Black BiModal Pipe Grade
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9485 g/cc0.03427 lb/in³Natural; ASTM D4883
 0.959 g/cc0.0346 lb/in³Black; ASTM D4883
Environmental Stress Crack Resistance >= 5000 hour>= 5000 hourCondition C; ASTM D1693
Carbon Black Loading 2.3 %2.3 %ASTM D1603
Melt Flow 8.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
8.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 10000 hour>= 10000 hourNotched Tensile; ASTM F1473
Hardness, Shore D 6666ASTM D2240
Tensile Strength at Break 37.9 MPa5500 psi2 in/min; ASTM D638
Tensile Strength, Yield 24.99 MPa3625 psi2 in/min; ASTM D638
Elongation at Break >= 600 %>= 600 %2 in/min; ASTM D638
Flexural Modulus 1.03 GPa
@Strain 2 %
150 ksi
@Strain 2 %
Secant - Method 1; ASTM D790
Izod Impact, Notched 4.81 J/cm9.00 ft-lb/inASTM D256
Hydrostatic Design Basis 6.89 MPa1000 psiat 60°C; ASTM D2837
 11.0 MPa
@Temperature 23.0 °C
1600 psi
@Temperature 73.4 °F
ASTM D2837
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 126 °C259 °FASTM D1525
Brittleness Temperature <= -118 °C<= -180 °FASTM D746
Decomposition Temperature >= 220 °C>= 428 °FThermal Stability; ASTM D2513/D3350
 
Descriptive Properties
Cell Classification445574C
processPipe Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos TUB 172 HDPE
Ineos TUB 121N HDPE
Ineos K38-20-160 Polyethylene Copolymer
Ineos TUB 121NTW HDPE
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade

PSOLKM017 / 89056

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.