MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos K38-20-188 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural gas distribution. The resulting formulation, known as K38-20X2091, is recognized by the Plastics Pipe Institute as having a PE 2708 (formerly PE 2406) and PE 80 rating. It exhibits excellent long term stress life and outstanding environmental stress crack resistance.

Cell Classification 234360D.

Key Words: A natural, UV stabilized, medium density polyethylene resin.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³Natural; ASTM D4883
Environmental Stress Crack Resistance >= 5000 hour>= 5000 hourCondition C; ASTM D1693
 >= 5000 hour>= 5000 hourPipe Ring; ASTM F1248
ESCR 10% Igepal® >= 5000 hour>= 5000 hourCondition B; ASTM D1693
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 500 hour>= 500 hourNotch Tensile; ASTM F1473
Hardness, Shore D 6464ASTM D2240
Tensile Strength, Ultimate 31.0 MPa4500 psi2 in/min; ASTM D638
Tensile Strength, Yield 19.3 MPa2800 psi2 in/min; ASTM D638
Elongation at Break >= 800 %>= 800 %2 in/min; ASTM D638
Flexural Modulus 0.689 GPa
@Strain 2 %
100 ksi
@Strain 2 %
Secant - Method 1; ASTM D790
Izod Impact, Notched 5.34 J/cm10.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 120 °C248 °FASTM D1525
Brittleness Temperature <= -118 °C<= -180 °FASTM D746
 
Descriptive Properties
processPipe Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos K38-20-160 Polyethylene Copolymer
Ineos TUB 172 HDPE
DSM Arnite® D04 300 PET (European Grade)
Ineos K44-06-122 HDPE
Ineos K44-08-122 HDPE

PSOLKF5 / 68223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.