MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nylene® Nylene BX3WQ662(X) Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Nylene BX3WQ662(X) is a advanced wire coating grade used for TH THHN Electrical Wire over PVC or as a standalone coating for copper or aluminum. High Speed Grade. Used in circuit sizes where high speed production is used (up to 2500mpm). Higher extractable levels (more flexibility).

Testing conducted on dry as molded specimen

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption <= 0.120 %<= 0.120 %Plant Test Method # 2-2B
Viscosity Measurement 2.65 - 2.95
@Temperature 20.0 °C
2.65 - 2.95
@Temperature 68.0 °F
Relative Viscosity; 96% Sulfuric Acid; Plant Test Method #2-5
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 0.0035 %0.0035 %35 ppm; Plant Test Method# 2-9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive
Taiwan Sheen Soon Sheenthane® AH-701 TPU for Hotmelt Adhesive
Parson Adhesives PARTITE® 7300 Methacrylate Structural Adhesive
Nylene® Nylene NX4795 Nylon 6

PNYLEN930 / 221462

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.