MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parson Adhesives PARTITE® 7300 Methacrylate Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: PARTITE 7300 is a two-component, 100% reactive, toughened structural methacrylate adhesive specifically formulated for bonding wide variety of metals, thermoplastics, thermosets, and composite assemblies.

FEATURE:

  • Convenient 1:1 mix ratio, Non-sagging and thixotropic formulation
  • Excellent impact, peel and shear resistance
  • Non-sagging, gaps filled up to 0.375 inches.
  • Room temperature cured with short open time.
APPLICATIONS:
  • Ideal for bonding all types of PVC, Polycarbonate, Acrylic, Fiberglass, PBT, PPO, ABS, FRT, Polyurethane, Epoxy, Wood, RIM, Nylon, FRP, Polyesters, Gelcoats, Styrene, Aluminum, CRS, Stainless Steel, Galvanized Steel, etc.
  • Ideal for Automotive Components, Marine Assemblies, Sporting goods, Electronics Enclosures, Appliances, Electrical Components, Furniture, Plastic Fabrications, Sign & Display, Metal Fabrications, etc.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0370 lb/in³Adhesive
 1.04 g/cc0.0377 lb/in³Activator
Brookfield Viscosity 40000 - 60000 cP40000 - 60000 cPRVT, Adhesive
 40000 - 60000 cP40000 - 60000 cPRVT, Activator
 90000 - 100000 cP90000 - 100000 cPMixed, Cure
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878ASTM D2240
Elongation at Break 19 %19 %
Shear Strength 10.3 MPa1500 psiABS/ABS, Substrate Failure; ASTM D1002
 11.7 MPa1700 psiFRP/FRP, Fiber Tear; ASTM D1002
 15.2 MPa2200 psiAluminum/ABS, Substrate Failure; ASTM D1002
 20.7 MPa3000 psi1 month immersion in Water @ 90°C; ASTM D1002
 21.68 MPa3145 psi1 month immersion in Water @ 23°C; ASTM D1002
 21.7 MPa3150 psi1 month immersion in Paraffin; ASTM D1002
 22.0 MPa3190 psiAluminum/Aluminum, Cohesive Failure; ASTM D1002
 22.0 MPa3190 psi1 month immersion in Acetic acid(10%); ASTM D1002
 22.1 MPa3200 psi1 month immersion in Xylene; ASTM D1002
 22.4 MPa3250 psi1 month immersion in Gasoline; ASTM D1002
 22.8 MPa3300 psi1 month immersion in Lubricating oil-HD30; ASTM D1002
 24.0 MPa3480 psiStainless steel/Stainless steel, Cohesive Failure; ASTM D1002
 27.2 MPa3950 psiEnvironmental Cycle, 30 days, Cohesive Failure; ASTM D1002
 29.0 MPa4200 psiDIN 53283
Tensile Impact 10.1 J/cm19.0 ft-lb/in
Peel Strength 3.16 kN/m18.0 pliStainless Steel/Stainless Steel, Average; ASTM D3807
 3.51 kN/m20.0 pliStainless Steel/Stainless Steel, Initial; ASTM D3807
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flash Point 51.0 °C124 °FAdhesive
 51.0 °C124 °FActivator
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull
Working Life 4.00 - 6.00 min4.00 - 6.00 min
 
Descriptive Properties
ColorMilky-WhiteAdhesive
 TanActivator
Gap Filling<0.375 inCured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Taiwan Sheen Soon Sheenthane® AH-701 TPU for Hotmelt Adhesive
Sinotek Materials Packing Expanded Graphite Yarns
Nylene® Nylene NX4795 Nylon 6
Nylene® Nylene BX3WQ662(X) Nylon 6

PPARSN090 / 186533

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.