MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parson Adhesives PARTITE® 7300 Methacrylate Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: PARTITE 7300 is a two-component, 100% reactive, toughened structural methacrylate adhesive specifically formulated for bonding wide variety of metals, thermoplastics, thermosets, and composite assemblies.

FEATURE:

  • Convenient 1:1 mix ratio, Non-sagging and thixotropic formulation
  • Excellent impact, peel and shear resistance
  • Non-sagging, gaps filled up to 0.375 inches.
  • Room temperature cured with short open time.
APPLICATIONS:
  • Ideal for bonding all types of PVC, Polycarbonate, Acrylic, Fiberglass, PBT, PPO, ABS, FRT, Polyurethane, Epoxy, Wood, RIM, Nylon, FRP, Polyesters, Gelcoats, Styrene, Aluminum, CRS, Stainless Steel, Galvanized Steel, etc.
  • Ideal for Automotive Components, Marine Assemblies, Sporting goods, Electronics Enclosures, Appliances, Electrical Components, Furniture, Plastic Fabrications, Sign & Display, Metal Fabrications, etc.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.55 lb/galAdhesive
 8.71 lb/galActivator
Brookfield Viscosity 40000 - 60000 cPRVT, Adhesive
 40000 - 60000 cPRVT, Activator
 90000 - 100000 cPMixed, Cure
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78ASTM D2240
Elongation at Break 19 %
Shear Strength 1500 psiABS/ABS, Substrate Failure; ASTM D1002
 1700 psiFRP/FRP, Fiber Tear; ASTM D1002
 2200 psiAluminum/ABS, Substrate Failure; ASTM D1002
 3000 psi1 month immersion in Water @ 90°C; ASTM D1002
 3145 psi1 month immersion in Water @ 23°C; ASTM D1002
 3150 psi1 month immersion in Paraffin; ASTM D1002
 3190 psiAluminum/Aluminum, Cohesive Failure; ASTM D1002
 3190 psi1 month immersion in Acetic acid(10%); ASTM D1002
 3200 psi1 month immersion in Xylene; ASTM D1002
 3250 psi1 month immersion in Gasoline; ASTM D1002
 3300 psi1 month immersion in Lubricating oil-HD30; ASTM D1002
 3480 psiStainless steel/Stainless steel, Cohesive Failure; ASTM D1002
 3950 psiEnvironmental Cycle, 30 days, Cohesive Failure; ASTM D1002
 4200 psiDIN 53283
Tensile Impact 19.0 ft-lb/in
Peel Strength 18.0 pliStainless Steel/Stainless Steel, Average; ASTM D3807
 20.0 pliStainless Steel/Stainless Steel, Initial; ASTM D3807
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -40.0 °F
Flash Point 51.0 °CAdhesive
 51.0 °CActivator
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull
Working Life 4.00 - 6.00 min
 
Descriptive Properties
ColorMilky-WhiteAdhesive
 TanActivator
Gap Filling<0.375 inCured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Taiwan Sheen Soon Sheenthane® AH-701 TPU for Hotmelt Adhesive
Sinotek Materials Packing Expanded Graphite Yarns
Nylene® Nylene NX4795 Nylon 6
Nylene® Nylene BX3WQ662(X) Nylon 6

PPARSN090 / 186533

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.