MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.

Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations, furniture, spraying, and fire hose co-extrusion.

Information provided by Taiwan Sheen Soon Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 300 - 600 cP300 - 600 cP15% solids in MEK
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 3.40 - 5.44 kN/m19.4 - 31.0 pliInitial (5 min.) PVC vs. PVC
 
Descriptive Properties
Activation temperature (°C)55-65
Heat Resistance, mm3070°C, PVC vs PVC
Max. Toluene in Solvents (%)30-35
Tack Time, min5 ~ 10PVC vs PVC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Taiwan Sheen Soon Sheenthane® AH-560 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-580 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-530 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-500 TPU for Hotmelt Adhesive

PSHEEN805 / 156209

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.