MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Elastosil® R 756/50 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R 756/50 is a peroxide curing high consistency silicone rubber whose vulcanizates possess excellent resistance to hot air, particularly after addition of heat stabilizer. The vulcanizates show good tear resistance, low compression set and are highly elastic.

Application: ELASTOSIL® R 756/50 is optimized for applications at high temperatures and can be used for molding applications. Vulcanizates of ELASTOSIL® R 756/50 in combination with ELASTOSIL® AUX Stabilizer, can withstand temperatures of 300 °C for at least seven days.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050curing Agent C1; DIN 53505
 52
@Treatment Temp. 250 °C,
Time 605000 sec
52
@Treatment Temp. 482 °F,
Time 168 hour
Hot air aged
 65
@Treatment Temp. 250 °C,
Time 3.46e+6 sec
65
@Treatment Temp. 482 °F,
Time 960 hour
Hot air aged
 76
@Treatment Temp. 300 °C,
Time 605000 sec
76
@Treatment Temp. 572 °F,
Time 168 hour
Hot air aged
Tensile Strength at Break 8.50 MPa1230 psicuring Agent C1; DIN 53504 S1
 4.80 MPa
@Treatment Temp. 300 °C,
Time 605000 sec
696 psi
@Treatment Temp. 572 °F,
Time 168 hour
Hot air aged
 6.20 MPa
@Treatment Temp. 250 °C,
Time 3.46e+6 sec
899 psi
@Treatment Temp. 482 °F,
Time 960 hour
Hot air aged
 6.80 MPa
@Treatment Temp. 250 °C,
Time 605000 sec
986 psi
@Treatment Temp. 482 °F,
Time 168 hour
Hot air aged
Elongation at Break 500 %500 %curing Agent C1; DIN 53504 S1
 130 %
@Treatment Temp. 300 °C,
Time 605000 sec
130 %
@Treatment Temp. 572 °F,
Time 168 hour
Hot air aged
 230 %
@Treatment Temp. 250 °C,
Time 3.46e+6 sec
230 %
@Treatment Temp. 482 °F,
Time 960 hour
Hot air aged
 400 %
@Treatment Temp. 250 °C,
Time 605000 sec
400 %
@Treatment Temp. 482 °F,
Time 168 hour
Hot air aged
Rebound 51 %51 %DIN 53512
Tear Strength 27.0 kN/m154 pliASTM D624 B
Compression Set 11 %
@Temperature 175 °C,
Time 79200 sec
11 %
@Temperature 347 °F,
Time 22.0 hour
DIN ISO 815-B
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
0.250 hour
@Treatment Temp. 329 °F
post cured 4h/200°C
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® R 420/70 Silicone Rubber
Wacker Elastosil® LR 3842/60 A/B Liquid Silicone Rubber
Wacker Elastosil® R plus 4806/20 Silicone Rubber
Wacker ELASTOSIL® R 427/70 High Strength Silicone Base
Wacker Elastosil® LR 3071/60 A/B Liquid Silicone Rubber

PWACK9236 / 204765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.