MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Elastosil® R 420/70 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R 420 silicone rubbers feature outstanding tear resistance and high transparency.

Application: In principle ELASTOSIL® R 420 silicone rubbers are designed for extrusion, compression, and transfer and injection molding. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183-1 A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6666curing agent E; DIN 53505
 7272curing agent C1; DIN 53505
Tensile Strength at Break 9.00 MPa1310 psicuring agent E; DIN 53504 S1
 10.0 MPa1450 psicuring agent C1; DIN 53504 S1
Elongation at Break 550 %550 %curing agent C1; DIN 53504 S1
 650 %650 %curing agent E; DIN 53504 S1
Rebound 40 %40 %curing agent E; DIN 53512
 46 %46 %curing agent C1; DIN 53512
Tear Strength 45.0 kN/m257 plicuring agent C1; ASTM D624 B
 48.0 kN/m274 plicuring agent E; ASTM D624 B
Compression Set  42 %
@Temperature 175 °C,
Time 79200 sec
42 %
@Temperature 347 °F,
Time 22.0 hour
curing agent C1; DIN ISO 815-B
 63 %
@Temperature 175 °C,
Time 79200 sec
63 %
@Temperature 347 °F,
Time 22.0 hour
curing agent E; DIN ISO 815-B
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Treatment Temp. 135 °C
0.167 hour
@Treatment Temp. 275 °F
curing agent E, press cured, 4hr/200°C
 15.0 min
@Treatment Temp. 165 °C
0.250 hour
@Treatment Temp. 329 °F
curing agent C1, press cured, 4hr/200°C
 15.0 min
@Treatment Temp. 165 °C
0.250 hour
@Treatment Temp. 329 °F
curing agent C6, press cured, 4hr/200°C
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3842/60 A/B Liquid Silicone Rubber
Wacker Elastosil® R 756/50 Silicone Rubber
Wacker Elastosil® R plus 4806/20 Silicone Rubber
Wacker Elastosil® LR 3071/60 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3005/60 A/B Liquid Silicone Rubber

PWACK9210 / 204739

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.