MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Elastosil® LR 3071/60 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Self-adhesive liquid silicone rubbers of the ELASTOSIL® LR 3071 series are paste-like, easily pigmentable two-component compounds with extremely short curing times.

ELASTOSIL® LR 3071 series are primerless, selfbonding grades that adhere to various plastic substrates (e.g. PA, PBT) and metals, but not in the mold (adhesive adherence, protects against loss prior to assembly). The bonding is improved by an ageing process (e.g. one hour at 100°C) or by a longer storing at room temperature. Because of the individual surface properties each substrate must be tested before mass production. If necessary one has to check the development of adhesive properties over time and/or in an environment relevant to the application. The vulcanizates are noted for good mechanical and electrical properties.

Application: ELASTOSIL® LR 3071 series are particularly suitable for the economical production of large series of overmolded parts (thermoplastic/elastomer), even in a comolding process (shuttle mold) under standard conditions, without any special treatment of the mold surface. Parts made from ELASTOSIL® LR 3071 can generally be used for technical applications without postcuring. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183-1 A
Viscosity  450000 cP
@Shear Rate 10.0 1/s
450000 cP
@Shear Rate 10.0 1/s
DIN 53019
 1.30e+6 cP
@Shear Rate 0.900 1/s
1.30e+6 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060DIN 53505
Tensile Strength at Break 8.50 MPa1230 psiDIN 53504 S 1
Elongation at Break 500 %500 %DIN 53504 S 1
Tear Strength 28.0 kN/m160 pliASTM 624 B
Compression Set  60 %
@Temperature 125 °C,
Time 79200 sec
60 %
@Temperature 257 °F,
Time 22.0 hour
DIN ISO 815-B
 70 %
@Temperature 150 °C,
Time 79200 sec
70 %
@Temperature 302 °F,
Time 22.0 hour
DIN ISO 815-B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 210 °C410 °Fwith heat stabilizer
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
in press
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cariflex IR0307 K Polyisoprene
Dow C6-570 LIQUID SILICONE RUBBER KIT
Dow Silastic® 7-6840 BIOMEDICAL GRADE LSR, KIT
Dow Silastic® 99-595-HC LIQUID SILICONE RUBBER KIT
Wacker Elastosil® LR 3842/60 A/B Liquid Silicone Rubber

PWACK9141 / 204670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.