MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Silicon Bronze, UNS C64200
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot formability. Fabricated by hot forming, forging, machining.

Applications: valve stems, gears, marine hardware, pole-line hardware, bolts, nuts, valve bodies and components.

Available as flat products and rod.

Key Words: CDA 642
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³C61400
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 517 - 703 MPa75000 - 102000 psi
Tensile Strength, Yield 241 - 469 MPa35000 - 68000 psiDepending on temper
Elongation at Break 32 %32 %in 558.8 mm.
Tensile Modulus 110 GPa16000 ksi
Machinability 60 %60 %UNS C36000 (free-cutting brass) = 100%
Forgeability 80 %80 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000220 ohm-cm0.0000220 ohm-cm8% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 3.75 W/m-K26.0 BTU-in/hr-ft²-°F
Melting Point 982 - 1000 °C1800 - 1840 °F
Solidus 982 °C1800 °F
Liquidus 1000 °C1840 °F
Annealing Point 593 - 704 °C1100 - 1300 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 7.0 %7.0 %
Copper, Cu 91.2 %91.2 %
Silicon, Si 1.8 %1.8 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed bar
Ampco Metal AMPCO® 642 Aluminum-Silicon-Copper Alloy, Extruded-Drawn-Stress Relieved (HR-50), ≤ 1/2"
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze
Free-Cutting Brass, UNS C36000
Aluminum-Silicon Bronze, UNS C95600, Copper Casting Alloy

MC64200b1 / 11628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.