MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum-Silicon Bronze, UNS C95600, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: Cable connectors, terminals, valve stems, marine hardware, gears, worms, pole-line hardware.

Classified under: Aluminum bronzes

Data typical for as-sand-cast separately cast test bars (M01 temper). Alloy does not respond to heat treating

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.69 g/cc0.278 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1401403000 kg
Tensile Strength, Ultimate 515 MPa74700 psi
Tensile Strength, Yield 235 MPa
@Strain 0.5 %
34100 psi
@Strain 0.5 %
Elongation at Break 18 %18 %in 50 mm
Modulus of Elasticity 105 GPa15200 ksi
Machinability 60 %60 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00002028 ohm-cm
@Temperature 20.0 °C
0.00002028 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.376 J/g-°C0.0899 BTU/lb-°F
Melting Point 982 - 1005 °C1800 - 1841 °F
Solidus 982 °C1800 °F
Liquidus 1005 °C1841 °F
Shrinkage 1.6 %1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 260 °C500 °FStress-Relieving Temperature
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 - 8.0 %6.0 - 8.0 %
Copper, Cu >= 88 %>= 88 %
Nickel, Ni <= 0.25 %<= 0.25 %
Silicon, Si 1.8 - 3.3 %1.8 - 3.3 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C95200, Copper Casting Alloy
Aluminum Bronze, UNS C95500, Casting Alloy, As-Cast
Aluminum Silicon Bronze, UNS C64200
Copper, UNS C62400 (Aluminum Bronze 11%)
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy

MC95600b1 / 11966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.