MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aluminum Silicon Bronze, UNS C64200
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot formability. Fabricated by hot forming, forging, machining.

Applications: valve stems, gears, marine hardware, pole-line hardware, bolts, nuts, valve bodies and components.

Available as flat products and rod.

Key Words: CDA 642
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.89 g/ccC61400
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 517 - 703 MPa
Tensile Strength, Yield 241 - 469 MPaDepending on temper
Elongation at Break 32 %in 558.8 mm.
Tensile Modulus 16000 ksi
Machinability 60 %UNS C36000 (free-cutting brass) = 100%
Forgeability 80 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000220 ohm-cm8% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 26.0 BTU-in/hr-ft²-°F
Melting Point 1800 - 1840 °F
Solidus 1800 °F
Liquidus 1840 °F
Annealing Point 1100 - 1300 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 7.0 %
Copper, Cu 91.2 %
Silicon, Si 1.8 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed bar
Ampco Metal AMPCO® 642 Aluminum-Silicon-Copper Alloy, Extruded-Drawn-Stress Relieved (HR-50), ≤ 1/2"
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze
Free-Cutting Brass, UNS C36000
Aluminum-Silicon Bronze, UNS C95600, Copper Casting Alloy

MC64200b1 / 11628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.