MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price/performance ratio and can be colored in almost any color. It does not cause any corrosion of or deposits on electrical contacts. Laser marking grades with a very good contrast are available.

Key characteristics:

  • UL 94 V2 at 0.75 mm
  • Halogen and red phosphorous free
  • Good overall mechanical performance
  • Low density
  • Colorable in a wide range of colors
  • Easy processing, fast cycling
  • No corrosion of or deposits on electrical contacts

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ASTM D792, ISO 1183
Water Absorption 1.0 %1.0 %23°C, 24h in H2O; sim. ISO 62
Water Absorption at Saturation 5.5 %5.5 %sim. ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inEuronil
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inEuronil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psiISO 527, ASTM D638
Elongation at Break 3.0 %3.0 %ISO 527, ASTM D638
Flexural Yield Strength 145 MPa21000 psiISO 178, ASTM D790
 95.0 MPa
@Temperature 90.0 °C
13800 psi
@Temperature 194 °F
ISO 178, ASTM D790
Flexural Modulus 7.60 GPa1100 ksiISO 178, ASTM D790
 3.25 GPa
@Temperature 90.0 °C
471 ksi
@Temperature 194 °F
ISO 178, ASTM D790
Izod Impact, Notched (ISO)  3.00 kJ/m²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²ISO 179
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 21.0 kV/mm
@Thickness 2.00 mm
533 kV/in
@Thickness 0.0787 in
ASTM D149
Comparative Tracking Index  550 V
@Thickness 3.20 mm
550 V
@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
 550 V
@Thickness 3.20 mm
550 V
@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 110 °C230 °F20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 191 °C376 °FISO 75, ASTM D648
Vicat Softening Point 210 °C410 °F49 N; ISO 306, ASTM D1525
 217 °C423 °F9.8 N; ISO 306, ASTM D1525
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
Oxygen Index 24 %24 %ASTM D2863
Glow Wire Flammability Index  960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 694-2-12
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 694-2-12
 
Descriptive Properties
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309
Needle TestOKIEC 695-2-2, 1 or 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Dry
Covestro Bayblend® FR3010 HF PC/ABS Blend
Celanese VECTRA® H130 30% Glass Filled Liquid Crystal Polymer (LCP)
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced

PLBN58 / 50447

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.