MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond UV15-7SP4 Low Shrinkage, One Component, UV Curable System
Categories: Polymer; Adhesive; Thermoset

Material Notes: Master Bond Polymer System UV15-7SP4 is a one component, low viscosity UV system with flexibility. UV15-7SP4 has very little shrinkage when curing and has non-yellowing properties. It bonds well to a wide variety of substrates including glass, metals and plastics, such as polycarbonates, acrylics and a number of films.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 800 - 1500 cP
@Temperature 23.0 °C
800 - 1500 cP
@Temperature 73.4 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3535
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
 
Descriptive Properties
ColorTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond UV15 One Component UV Curable Epoxy
Master Bond UV15-7 One Part UV Curable Polymer
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy

PMASTB124 / 52281

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.