MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Elexar® EL 8730R Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar® EL-8730R is high performance, flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar® EL-8730A is a high durometer grade that is UV stabilized and RoHS compliant. This grade is UL listed and is suitable for both injection molding and extrusion.

Features: Flame Retardant; General Purpose; Good Colorability; Good Flexibility; Halogenated; High Elasticity; High Elongation; High Tensile Strength; Medium Flow; Ozone Resistant; Sunlight Resistant (720 hours); UV Resistant; Weather Resistant

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
13 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ASTM D2240
Tensile Strength at Break 13.4 MPa
@Thickness 0.508 mm
1940 psi
@Thickness 0.0200 in
Extruded Tape, Die C, 20 in/min; ASTM D412
 13.26 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
1923 psi
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 14.74 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
2138 psi
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
Tensile Stress at Strain  4.55 MPa
@Strain 100 %,
Thickness 0.508 mm
660 psi
@Strain 100 %,
Thickness 0.0200 in
Extruded Tape, Die C, 20 in/min; ASTM D412
 6.48 MPa
@Strain 300 %,
Thickness 0.508 mm
940 psi
@Strain 300 %,
Thickness 0.0200 in
Extruded Tape, Die C, 20 in/min; ASTM D412
Elongation at Break 620 %
@Thickness 0.508 mm
620 %
@Thickness 0.0200 in
Extruded Tape, Die C, 20 in/min; ASTM D412
 595.2 %
@Treatment Temp. 136 °C,
Time 605000 sec
595.2 %
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
 638.6 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
638.6 %
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant  2.32
@Frequency 1e+6 Hz
2.32
@Frequency 1e+6 Hz
ASTM D150
 2.36
@Frequency 1000 Hz
2.36
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 38.6 kV/mm980 kV/inASTM D418
Dissipation Factor  0.0011
@Frequency 1000 Hz
0.0011
@Frequency 1000 Hz
ASTM D150
 0.0016
@Frequency 1e+6 Hz
0.0016
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FUL 1581
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
Flammability, UL94  V-2
@Thickness 1.52 mm
V-2
@Thickness 0.0600 in
All Colors
 V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0600 in
NT, ST, BK
Oxygen Index 25 %25 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer
Teknor Apex Elexar® EL 1934F Thermoplastic Elastomer
Teknor Apex Monprene® MP 1304 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1544 Thermoplastic Elastomer

PTEKNO783 / 128964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.