MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Elexar® EL 1934F Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar® EL-1934F is a high performance UL V-0 flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar EL-1934F is a high hardness, high density, high flow grade that is UV stabilized and RoHS compliant. This UL listed grade is easily colorable and is suitable for both molding and extrusion.

Features: Brominated; Electrically Insulating; Flame Retardant; Good Colorability; Good Flexibility; Halogenated; High Density; High Flow; High Specific Gravity; Medium Hardness; Sunlight Resistant (720 hours); UV Resistant

Uses: Cable Jacketing; Connectors; Insulation; Wire & Cable Applications

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 9.65 MPa1400 psiDie C, 20 in/min; ASTM D412
 8.11 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
1180 psi
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 10.13 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
1469 psi
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
Elongation at Break 600 %600 %Die C, 20 in/min; ASTM D412
 576 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
576 %
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 588 %
@Treatment Temp. 136 °C,
Time 605000 sec
588 %
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.3
@Frequency 1000 Hz
2.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 38.2 kV/mm970 kV/inASTM D149
Dissipation Factor 0.0030
@Frequency 1000 Hz
0.0030
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FUL 1581
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
Flammability, UL94 V-0V-0
Oxygen Index 3.0 %3.0 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 199 - 216 °C390 - 420 °F
Middle Barrel Temperature 213 - 221 °C415 - 430 °F
Front Barrel Temperature 221 - 227 °C430 - 440 °F
Nozzle Temperature 221 - 229 °C430 - 445 °F
Zone 1 193 - 210 °C380 - 410 °F
Zone 2 199 - 216 °C390 - 420 °F
Zone 3 213 - 221 °C415 - 430 °F
Zone 4 216 - 221 °C420 - 430 °F
Zone 5 221 - 227 °C430 - 440 °F
Die Temperature 221 - 229 °C430 - 445 °F
Melt Temperature 221 - 229 °C430 - 445 °FProcessing Temp
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer
Saint-Gobain Tygon® PT-3350 Sanitary Silicone Tubing Formulation
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer

PTEKNO774 / 128955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.