MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Notes: Telcar TL-1934E is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Telcar TL-1934E is a high hardness, high density grade that is UL 94 rated with 720hr sunlight resistance. This grade is suitable for both injection molding and extrusion.

Features: Brominated; Flame Retardant; General Purpose; Good Colorability; Good Flexibility; Halogenated; High Hardness; High Specific Gravity; Low Flow; Slip; Sunlight Resistant (720 hrs); UV Resistant

Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Core Insulation; Wire & Cable Application; Wire Jacketing

Form: Pellets

Processing Method: Injection Molding; Extrusion

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TES
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 200 °C
18 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383ASTM D2240
Tensile Strength at Break 8.5909 MPa1246.0 psiChange in tensile strength in air after 168 hours at 316°F; ASTM D573
 9.267 MPa1344 psiChange in tensile strength in air after 3600 hours at 268°F; ASTM D573
 9.65 MPa1400 psi20 in/min; ASTM D412
 8.50 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
1230 psi
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 9.65 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
1400 psi
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
Elongation at Break 462.0 %462.0 %After aging in air 3600 hours at 268°F; ASTM D573
 467.5 %467.5 %After aging in air 168 hours at 316°F; ASTM D573
 550 %550 %20 in/min; ASTM D412
 495 %
@Treatment Temp. 136 °C,
Time 605000 sec
495 %
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D471
 495 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
495 %
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.42.4ASTM D150
Dielectric Strength 35.4 kV/mm900 kV/inASTM D419
Dissipation Factor 0.00400.0040ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FContinuous; UL 1581
Brittleness Temperature -59.0 °C-74.2 °FASTM D746
UL RTI, Electrical 50.0 °C122 °FUL 746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746
Flammability, UL94 V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0600 in
QMFZ2.E54709; QMTT2.E73402
Oxygen Index 26 %26 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 193 °C340 - 380 °F
Middle Barrel Temperature 177 - 199 °C350 - 390 °F
Front Barrel Temperature 182 - 204 °C360 - 400 °F
Nozzle Temperature 188 - 210 °C370 - 410 °F
Zone 1 166 - 188 °C330 - 370 °F
Zone 2 171 - 193 °C340 - 380 °F
Zone 3 177 - 199 °C350 - 390 °F
Zone 5 182 - 204 °C360 - 400 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 188 - 210 °C370 - 410 °FProcessing Temperature
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Elexar® EL 8730R Thermoplastic Elastomer
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer
Teknor Apex Elexar® EL 1934F Thermoplastic Elastomer
Teknor Apex ELEXAR® EL 8451 Thermoplastic Elastomer

PTEKNP567 / 129640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.