MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo EMERGE™ 8702 Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: EMERGE™ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC resin with a mold release system, intended for injection molding applications.

Applications:

  • Information Technology Equipment
  • Electrical Parts
  • Other structural/internal parts

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D955
Melt Flow 5.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
5.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 100 MPa14500 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Tensile Modulus 6.00 GPa870 ksiASTM D638
Flexural Strength 170.0 MPa24650 psiASTM D790
Flexural Modulus 5.499 GPa797.5 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm
@Thickness 1.80 mm
1.00e+16 ohm-cm
@Thickness 0.0709 in
ASTM D257
Surface Resistance 3.00e+14 ohm3.00e+14 ohmASTM D257
Dielectric Constant 3.1
@Thickness 1.60 mm,
Frequency 10 - 1.00e+6 Hz
3.1
@Thickness 0.0630 in,
Frequency 10 - 1.00e+6 Hz
ASTM D150
Dielectric Strength >= 27.2 kV/mm
@Thickness 1.60 mm
>= 692 kV/in
@Thickness 0.0630 in
ASTM D149
Dissipation Factor  0.0025
@Frequency 100 Hz
0.0025
@Frequency 100 Hz
ASTM D150
 0.0050
@Frequency 10 Hz
0.0050
@Frequency 10 Hz
ASTM D150
 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 175 V
@Thickness 3.00 mm
175 V
@Thickness 0.118 in
IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.2 µm/m-°C
@Temperature -40.0 - 82.2 °C
14.0 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
CTE, linear, Transverse to Flow 52.2 µm/m-°C
@Temperature -40.0 - 82.2 °C
29.0 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
Hot Ball Pressure Test >= 135 °C>= 275 °FIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °Funannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °C284 °Funannealed; ASTM D648
 143 °C289 °Fannealed; ASTM D648
Vicat Softening Point 150 °C302 °F50°C/hr, 50N; ASTM D1525
 160 °C320 °F120°C/hr, 10N; ASTM D1525
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 35 %35 %ASTM D2863
Glow Wire Test 960 °C
@Thickness 1.00 - 3.00 mm
1760 °F
@Thickness 0.0394 - 0.118 in
IEC 60695-2-10

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 5101-15 Polycarbonate Resin
Trinseo EMERGE™ PC 8701-15 Polycarbonate Resin
Trinseo CALIBRE™ 5101-8 Polycarbonate Resin
Trinseo EMERGE™ PC 8702-15 (AP) Polycarbonate Resin
Trinseo EMERGE™ PC 8130-10 Polycarbonate Resin

PZZDOW1337 / 30555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.