EMERGE™ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced polycarbonate resin. This resin contains no bromine, chlorine or phosphate additives. It is a medium flow PC resin with a mold release system, intended for applications requiring high stiffness. It has a UL94 flammability rating of V-0 at 1.5 mm. Main Characteristics: - Glass reinforced
- Ignition resistant
Applications:- Powered Device Housings
- Information technology equipment
- Electrical parts
- Other structural/internal parts
Information provided by Trinseo. |