MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ PC 8702-15 (AP) Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: EMERGE™ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced polycarbonate resin. This resin contains no bromine, chlorine or phosphate additives. It is a medium flow PC resin with a mold release system, intended for applications requiring high stiffness. It has a UL94 flammability rating of V-0 at 1.5 mm.

Main Characteristics:

  • Glass reinforced
  • Ignition resistant
Applications:
  • Powered Device Housings
  • Information technology equipment
  • Electrical parts
  • Other structural/internal parts

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0040 in/inISO 294-4
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Elongation at Break 4.0 %
@Thickness 3.20 mm
Injection Molded; ASTM D638
Tensile Modulus 4000 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Izod Impact, Notched 110 J/m
@Temperature 3.20 °C
Injection Molded; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
@Thickness 1.80 mm
ASTM D257
Surface Resistance 3.00e+14 ohmASTM D257
Dielectric Constant 3.1
@Thickness 1.60 mm,
Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 27.0 kV/mm
@Thickness 1.60 mm
ASTM D149
Comparative Tracking Index 175 V
@Thickness 3.00 mm
IEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 145 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °CUnannealed; ASTM D648
 143 °CAnnealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 288 - 316 °C
Mold Temperature 79.0 - 116 °C
Drying Temperature 121 °C
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ PC 8701-15 Polycarbonate Resin
Trinseo EMERGE™ 8600-20 Polycarbonate
Trinseo EMERGE™ 8702 Polycarbonate
Trinseo EMERGE™ PC 8130-15 Polycarbonate Resin
Trinseo PULSE™ GX50 PC/ABS Engineering Resin

PTRINS9048 / 197547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.