MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo EMERGE™ PC 8130-10 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: EMERGE™ PC 8130 Advanced Resin is a specially designed ignition-resistant polycarbonate resin with improved UV stability. It is designed for thin-wall applications and has a UL94 V-0 rating 1.0 mm. EMERGE PC 8130 is also f1 rated according to UL 746C. This material does not contain chlorine or bromine additives.

Main Characteristics:

  • Ignition resistant
  • UV resistant
Applications:
  • Powder Device Housings
  • Information technology equipment
  • Electrical parts

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 58.6 MPa8500 psiASTM D638
 59.0 MPa8560 psiISO 527-2/50
Tensile Strength, Yield 61.0 MPa8850 psiISO 527-2/50
 61.4 MPa8910 psiASTM D638
Elongation at Break 120 %120 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.38 GPa345 ksiASTM D638
Flexural Strength 97.9 MPa14200 psiASTM D790
Flexural Modulus 2.33 GPa338 ksiASTM D790
Izod Impact, Notched 6.90 J/cm12.9 ft-lb/inASTM D256
Tensile Impact Strength 630 kJ/m²300 ft-lb/in²ASTM D1822
Dart Drop, Total Energy 62.1 J45.8 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance <= 60 sec<= 60 secASTM D495
High Voltage Arc Resistance to Ignition (HVAR) 120 - 300 sec120 - 300 sec
Comparative Tracking Index 250 - 399 V250 - 399 VUL 746
Hot Wire Ignition, HWI 30 - 59 sec
@Diameter 0.900 - 3.00 mm
30 - 59 sec
@Diameter 0.0354 - 0.118 in
UL 746
High Amp Arc Ignition, HAI  30 - 59 arcs
@Thickness 0.900 mm
30 - 59 arcs
@Thickness 0.0354 in
UL 746
 60 - 119 arcs
@Thickness 1.00 - 3.00 mm
60 - 119 arcs
@Thickness 0.0394 - 0.118 in
UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C36.1 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
@Thickness 6.40 mm
261 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 151 °C304 °FASTM D1525
UL RTI, Electrical 130 °C266 °FUL 746
UL RTI, Mechanical with Impact 115 °C239 °FUL 746
UL RTI, Mechanical without Impact 130 °C266 °FUL 746
Flammability, UL94  V-1
@Thickness 0.900 mm
V-1
@Thickness 0.0354 in
all
 V-0
@Thickness 0.900 mm
V-0
@Thickness 0.0354 in
wt, black
 V-0
@Thickness 1.00 mm
V-0
@Thickness 0.0394 in
all
 5VB
@Thickness 2.00 mm
5VB
@Thickness 0.0787 in
all
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
all
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 302 °C550 - 576 °F
Drying Temperature 121 °C250 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo EMERGE™ PC 8130-15 Polycarbonate Resin
Entec Hylex® P1310FR Polycarbonate
Ineos H20H-00 Polypropylene Homopolymer
Trinseo CALIBRE™ 893-10 Polycarbonate
Trinseo EMERGE™ 4330-15 Polycarbonate

PTRINS9044 / 197544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.