MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EXACT™ 8210 Plastomer for Polymer Modification  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene octene copolymer produced using ExxonMobil Chemical Exxpol technology, exhibiting both plastic and elastomeric properties. Designed for modification of both polypropylenes and polyethylenes in applications such as injection molding, cast film, and profile extrusion.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.882 g/cc0.0319 lb/in³ExxonMobil Method
Mooney Viscosity 5.9
@Temperature 125 °C
5.9
@Temperature 257 °F
ML (1 + 4); ASTM D1646
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 25 g/10 min25 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 797915s; ASTM D2240
Hardness, Shore D 272715s; ASTM D2240
Tensile Stress at Strain  2.81 MPa
@Strain 100 %
407 psi
@Strain 100 %
ASTM D412
 3.40 MPa
@Strain 300 %
493 psi
@Strain 300 %
ASTM D412
Flexural Modulus, 1% Secant 26.25 MPa3807 psiASTM D790
Izod Impact, Notched NBNBASTM D256
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D256
Instrumented Impact Total Energy  17.2 J
@Temperature 23.0 °C
12.7 ft-lb
@Temperature 73.4 °F
ASTM D3763
 25.9 J
@Temperature -40.0 °C
19.1 ft-lb
@Temperature -40.0 °F
ASTM D3763
Instrumented Impact Energy at Peak  12.5 J
@Temperature 23.0 °C
9.20 ft-lb
@Temperature 73.4 °F
ASTM D3763
 15.3 J
@Temperature -40.0 °C
11.3 ft-lb
@Temperature -40.0 °F
ASTM D3763
Tear Strength 43.1 kN/m246 pliDie C; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 73.72 °C164.7 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 71.00 °C159.8 °Fat 200g; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 13 %
@Thickness 1.27 mm
13 %
@Thickness 0.0500 in
ASTM D1003
 
Descriptive Properties
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 3035 Plastomer for Polymer Modification
ExxonMobil EXACT™ 230 Plastomer for Polymer Modification
ExxonMobil EXACT™ 210 Plastomer for Polymer Modification
ExxonMobil EXACT™ 203 Plastomer for Polymer Modification
ExxonMobil EXACT™ 201 Plastomer for Polymer Modification

PEXB375 / 37680

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.