MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EXACT™ 201 Plastomer for Polymer Modification  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene octene copolymer produced using ExxonMobil Chemical Exxpol technology, exhibiting both plastic and elastomeric properties. Designed for modification of both polypropylenes and polyethylenes in applications such as injection molding, extrusion blow molding, blown and cast film, and profile extrusion.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ExxonMobil Method
Mooney Viscosity 3.9
@Temperature 125 °C
3.9
@Temperature 257 °F
ML (1 + 4); ASTM D1646
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourCondition A; ASTM D1693
Melt Flow 1.1 g/10 min1.1 g/10 minASTM D1238
 2.5 g/10 min2.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 90>= 9015s; ASTM D2240
Hardness, Shore D 36.836.815s; ASTM D2240
Tensile Strength, Ultimate 30.71 MPa4454 psiASTM 412
Tensile Stress at Strain  12.3 MPa
@Strain 100 %
1780 psi
@Strain 100 %
ASTM D412
 14.58 MPa
@Strain 300 %
2115 psi
@Strain 300 %
ASTM D412
Elongation at Break 1144 %1144 %ASTM D412
Flexural Modulus, 1% Secant 67.86 MPa9842 psiASTM D790
Izod Impact, Notched NBNBASTM D256
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D256
Instrumented Impact Total Energy  33.8 J
@Temperature -40.0 °C
24.9 ft-lb
@Temperature -40.0 °F
ASTM D3763
 40.8 J
@Temperature 23.0 °C
30.1 ft-lb
@Temperature 73.4 °F
ASTM D3763
Instrumented Impact Energy at Peak  17.6 J
@Temperature -40.0 °C
13.0 ft-lb
@Temperature -40.0 °F
ASTM D3763
 20.6 J
@Temperature 23.0 °C
15.2 ft-lb
@Temperature 73.4 °F
ASTM D3763
Tear Strength 89.1 kN/m508 pliDie C; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 96.89 °C206.4 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 83.72 °C182.7 °Fat 1000g; ASTM D1525
 96.22 °C205.2 °Fat 200g; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 76.1 %
@Thickness 1.02 mm
76.1 %
@Thickness 0.0400 in
ASTM D1003
 
Descriptive Properties
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 0201FX Plastomer for Blown Film Applications
Dow Engage® 8003 Polyolefin Elastomer
ExxonMobil EXACT™ 201 Plastomer for Blown Film Applications
ExxonMobil EXACT™ 3035 Plastomer for Polymer Modification
ExxonMobil EXACT™ 8210 Plastomer for Polymer Modification

PEXB358 / 37663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.