MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EXACT™ 230 Plastomer for Polymer Modification  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene octene copolymer produced using ExxonMobil Chemical Exxpol technology, exhibiting both plastic and elastomeric properties. Designed for modification of both polypropylenes and polyethylenes in applications such as injection molding, cast film, and profile extrusion.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ExxonMobil Method
Melt Flow 30 g/10 min30 g/10 minASTM D1238
 65.1 g/10 min65.1 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 888815s; ASTM D2240
Hardness, Shore D 393915s; ASTM D2240
Tensile Strength at Break 11.3 MPa1640 psiASTM D638
Tensile Strength, Ultimate 11.3 MPa1640 psiASTM 412
Tensile Stress at Strain  6.500 MPa
@Strain 300 %
942.8 psi
@Strain 300 %
ASTM D412
 6.800 MPa
@Strain 100 %
986.3 psi
@Strain 100 %
ASTM D412
Elongation at Break 1679 %1679 %ASTM D638
 1679 %1679 %ASTM D412
Flexural Modulus, 1% Secant 79.50 MPa11530 psiASTM D790
Izod Impact, Notched NBNBASTM D256
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D256
Instrumented Impact Total Energy  14.9 J
@Temperature 23.0 °C
11.0 ft-lb
@Temperature 73.4 °F
ASTM D3763
 26.6 J
@Temperature -40.0 °C
19.6 ft-lb
@Temperature -40.0 °F
ASTM D3763
Instrumented Impact Energy at Peak  7.32 J
@Temperature 23.0 °C
5.40 ft-lb
@Temperature 73.4 °F
ASTM D3763
 16.4 J
@Temperature -40.0 °C
12.1 ft-lb
@Temperature -40.0 °F
ASTM D3763
Tear Strength 430.7 kN/m2458 pliDie C; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 95.39 °C203.7 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 91.89 °C197.4 °Fat 200g; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 90 %
@Thickness 1.27 mm
90 %
@Thickness 0.0500 in
ASTM D1003
 
Descriptive Properties
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 3035 Plastomer for Polymer Modification
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
ExxonMobil EXACT™ 8210 Plastomer for Polymer Modification
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
ExxonMobil EXACT™ 5731 Plastomer for Polymer Modification

PEXB361 / 37666

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.