MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.29 - 1.70 g/cc0.0466 - 0.0614 lb/in³Average value: 1.53 g/cc Grade Count:11
Water Absorption 0.0300 - 0.300 %0.0300 - 0.300 %Average value: 0.127 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.00500 cm/cm0.00100 - 0.00500 in/inAverage value: 0.00309 cm/cm Grade Count:11
Linear Mold Shrinkage, Transverse 0.00500 - 0.00600 cm/cm0.00500 - 0.00600 in/inAverage value: 0.00550 cm/cm Grade Count:4
Spiral Flow 25.0 - 25.0 cm
@Temperature 300 - 300 °C
9.84 - 9.84 in
@Temperature 572 - 572 °F
Average value: 25.0 cm Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115 - 120115 - 120Average value: 119 Grade Count:5
Tensile Strength, Ultimate 112 - 195 MPa16200 - 28300 psiAverage value: 150 MPa Grade Count:11
Elongation at Break 1.40 - 5.00 %1.40 - 5.00 %Average value: 3.03 % Grade Count:11
Flexural Yield Strength 202 - 275 MPa29300 - 39900 psiAverage value: 224 MPa Grade Count:11
Flexural Modulus 9.30 - 22.0 GPa1350 - 3190 ksiAverage value: 14.4 GPa Grade Count:11
Compressive Yield Strength 195 - 225 MPa28300 - 32600 psiAverage value: 211 MPa Grade Count:4
Izod Impact, Notched 0.430 - 1.00 J/cm0.806 - 1.87 ft-lb/inAverage value: 0.731 J/cm Grade Count:11
Izod Impact, Unnotched 1.60 - 8.00 J/cm3.00 - 15.0 ft-lb/inAverage value: 4.41 J/cm Grade Count:11
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.80 - 4.503.80 - 4.50Average value: 4.05 Grade Count:5
Dielectric Strength 17.0 - 27.0 kV/mm432 - 686 kV/inAverage value: 23.0 kV/mm Grade Count:5
Dissipation Factor 0.00200 - 0.03000.00200 - 0.0300Average value: 0.0136 Grade Count:5
Arc Resistance 100 - 116 sec100 - 116 secAverage value: 108 sec Grade Count:4
Comparative Tracking Index 150 - 275 V150 - 275 VAverage value: 225 V Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 - 22.0 µm/m-°C10.0 - 12.2 µin/in-°FAverage value: 20.0 µm/m-°C Grade Count:4
 18.0 - 39.0 µm/m-°C
@Temperature 100 - 200 °C
10.0 - 21.7 µin/in-°F
@Temperature 212 - 392 °F
Average value: 28.5 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 50.0 - 63.0 µm/m-°C27.8 - 35.0 µin/in-°FAverage value: 56.5 µm/m-°C Grade Count:4
 92.0 - 110 µm/m-°C
@Temperature 100 - 200 °C
51.1 - 61.1 µin/in-°F
@Temperature 212 - 392 °F
Average value: 101 µm/m-°C Grade Count:4
Melting Point 280 - 290 °C536 - 554 °FAverage value: 284 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 250 - 271 °C482 - 520 °FAverage value: 261 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 229 - 260 °C444 - 500 °FAverage value: 246 °C Grade Count:11
Flammability, UL94 V-0V-0Grade Count:3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 299 - 330 °C570 - 626 °FAverage value: 308 °C Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Thermoset Polyester, Mineral Filled
Overview of materials for Polyphenylene Sulfide (PPS); Molded
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler

O4510 / 78337

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.