MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Heligoen® Blue L 6700 F Color Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Structure: Cu-phthalocyanine, Epsilon

Application: Pigment for Paints

Physical form: Powder

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³
Specific Surface Area 54 m²/g54 m²/g
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 5.0 - 8.05.0 - 8.0
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 5000 ohm-cm>= 5000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 350 °C662 °F
 
Descriptive Properties
Chemical Fastness (months)Butyl Acetate3-4
 Ethanol4
 Methyl ethyl ketone2
 Mineral spirits5
 Solvenon™PM3-4
 Xylene3
ColorBlue
Fastness to OvercoatingAcid Resistance5
 Alkali Resistance5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Z-6701 SILANE
Teknor Apex TEKBOND® 6700-65 Thermoplastic Elastomer
Solvay BR® 6700-1 Bonding Primer
Rogers Arlon CuClad 6700 Bonding Film
Covestro DESMODUR® TT163 + BAYTEC® XL 1705, 93 A Polyurethane, TDI- PTMEG

PBASG0711 / 132344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.