System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
BASF Heligoen® Blue L 6700 F Color Additive
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
Material Notes:
Chemical Structure: Cu-phthalocyanine, Epsilon
Application: Pigment for Paints
Physical form: Powder
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.68
g/cc
Specific Surface Area
54
m²/g
Chemical Properties
Original Value
Comments
Total Acid Number
5.0 - 8.0
Electrical Properties
Original Value
Comments
Electrical Resistivity
>=
5000
ohm-cm
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
350
°C
Descriptive Properties
Chemical Fastness (months)
Butyl Acetate
3-4
Ethanol
4
Methyl ethyl ketone
2
Mineral spirits
5
Solvenon™PM
3-4
Xylene
3
Color
Blue
Fastness to Overcoating
Acid Resistance
5
Alkali Resistance
5
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Dow Z-6701 SILANE
Teknor Apex TEKBOND® 6700-65 Thermoplastic Elastomer
Solvay BR® 6700-1 Bonding Primer
Rogers Arlon CuClad 6700 Bonding Film
Covestro DESMODUR® TT163 + BAYTEC® XL 1705, 93 A Polyurethane, TDI- PTMEG
PBASG0711 / 132344
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.