MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA217080 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Applications
PETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation.

Processing Techniques
NA 217-080, like other thermoplastic polyolefin resins, can be extruded as wire and cable insulation by means a conventional extruder. Below are suggested extrusion conditions for NA 217-080. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size have an effect on the processing of thermoplastic resins.

This product is from the former Equistar product line.

Key Words: LDPE; Fiber Optic/Coaxial; Insulation
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 5.6 g/10 min5.6 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353ASTM D2240
Tensile Strength at Break 12.4 MPa1800 psiASTM D638
Tensile Strength, Yield 10.3 MPa1500 psiASTM D638
Elongation at Break 550 %550 %ASTM D638
Flexural Modulus, 1% Secant 276 MPa40000 psiASTM D790
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.28
@Frequency 1e+6 Hz
2.28
@Frequency 1e+6 Hz
ASTM D1531
Dissipation Factor  0.000040
@Frequency 1e+6 Hz
0.000040
@Frequency 1e+6 Hz
ASTM D1531
 0.000040
@Frequency 2.00e+9 Hz
0.000040
@Frequency 2.00e+9 Hz
ASTM D1531
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746
 
Processing PropertiesMetricEnglishComments
Feed Temperature 138 - 149 °C280 - 300 °F
Zone 2 149 - 163 °C300 - 325 °F
Zone 3 191 - 204 °C375 - 400 °F
Zone 4-x 204 - 218 °C400 - 425 °F
Adapter Temperature 204 - 218 °C400 - 425 °F
Die Temperature 204 - 218 °C400 - 425 °F
Melt Temperature 204 - 218 °C400 - 425 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FA6220 Low Density Polyethylene
Westlake EC850AA Low Density Polyethylene
LyondellBasell Petrothene® NA217000 Low Density Polyethylene
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene
Röchling Polystone® G natural PE-HD

PEQU0273 / 36707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.