MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0.7% copper additions combined with the chromium and molybdenum additions improve the behavior of the steel in many corrosive solutions encountered for example in chemical and petrochemical processes or chloride containing solutions. The alloy is also seawater resistant and has extensively been used in offshore industries (It has not to be used in stagnant seawater application with temperatures higher than 30° 86°F). Thanks to the 18% Nickel and the 0.2 Nitrogen additions, the microstructure is austenitic.

Information provided by manufacturer.

Key Words: EURONORM X1 Cr Ni Mo Cu N 20.18.7, AFNOR Z2 CNDU 20.18.7 Az, DIN W.Nr 1.4547, ASTM UNS S31254
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 190 - 230190 - 230Typical, V10
Tensile Strength, Ultimate >= 650 MPa>= 94300 psiMinimum Guaranteed
Tensile Strength, Yield  >= 300 MPa
@Strain 0.2 %
>= 43500 psi
@Strain 0.2 %
 >= 330 MPa
@Strain 1 %
>= 47900 psi
@Strain 1 %
Elongation at Break >= 35 %>= 35 %
Modulus of Elasticity 195 GPa28300 ksi
Poissons Ratio 0.300.30Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
10900 ksi
@Temperature 68.0 °F
Charpy Impact >= 60.0 J
@Temperature -196 °C
>= 44.3 ft-lb
@Temperature -321 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000900 ohm-cm
@Temperature 20.0 °C
0.0000900 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.5 µm/m-°C
@Temperature 20.0 - 100 °C
9.17 µin/in-°F
@Temperature 68.0 - 212 °F
 17.0 µm/m-°C
@Temperature 20.0 - 300 °C
9.44 µin/in-°F
@Temperature 68.0 - 572 °F
 17.3 µm/m-°C
@Temperature 20.0 - 500 °C
9.61 µin/in-°F
@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.480 J/g-°C
@Temperature 20.0 °C
0.115 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 13.0 W/m-K
@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 %0.010 %
Chromium, Cr 20 %20 %
Copper, Cu 0.70 %0.70 %
Iron, Fe 54.989 %54.989 %As remainder
Molybdenum, Mo 6.1 %6.1 %
Nickel, Ni 18 %18 %
Nitrogen, N 0.20 %0.20 %
Sulfur, S 0.0010 %0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
MetalTek 254 SMO® Super Austenitic Stainless Steel
Carlson 926 Mo Austenitic Stainless Steel
MetalTek MTEK 6XN Cast UNS J94651 Super Austenitic Stainless Steel
Outokumpu 4529 Austenitic Stainless Steel

NINDUST42 / 17580

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.