MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Outokumpu 4529 Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes:

Applications: Wet corrosion resistance and general service.

Available in hot rolled plate (Quarto) form.

Key Words: EN 1.4529; UNS N08926
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.10 g/cc0.293 lb/in³RT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 750 MPa109000 psiOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield  300 MPa
@Strain 0.2 %
43500 psi
@Strain 0.2 %
EN min., RT; EN 10002-1
 360 MPa
@Strain 0.2 %
52200 psi
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 430 MPa
@Strain 1 %
62400 psi
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 160 MPa
@Strain 0.2 %,
Temperature 400 °C
23200 psi
@Strain 0.2 %,
Temperature 752 °F
EN min.; EN 10002-5
 190 MPa
@Strain 0.2 %,
Temperature 200 °C
27600 psi
@Strain 0.2 %,
Temperature 392 °F
EN min.; EN 10002-5
 230 MPa
@Strain 0.2 %,
Temperature 100 °C
33400 psi
@Strain 0.2 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 55 %55 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 195 GPa28300 ksiRT
 166 GPa
@Temperature 400 °C
24100 ksi
@Temperature 752 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000100 ohm-cm0.000100 ohm-cmRT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.8 µm/m-°C
@Temperature 100 °C
8.78 µin/in-°F
@Temperature 212 °F
 16.9 µm/m-°C
@Temperature 400 °C
9.39 µin/in-°F
@Temperature 752 °F
Specific Heat Capacity 0.450 J/g-°C0.108 BTU/lb-°FRT
Thermal Conductivity 12.0 W/m-K83.3 BTU-in/hr-ft²-°FRT
 18.0 W/m-K
@Temperature 400 °C
125 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Chromium, Cr 20 %20 %
Copper, Cu 0.50 %0.50 %
Iron, Fe 48 %48 %as balance
Molybdenum, Mo 6.5 %6.5 %
Nickel, Ni 25 %25 %
Nitrogen, N 0.20 %0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlson 926 Mo Austenitic Stainless Steel
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Crucible Steel SUE52 Martensitic Steel
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42

NOUTOK33 / 18748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.