Corrosion resistance approaching nickel alloys, especially in chloride service. Produced under license of Avesta Jernverk AB. Applications: Process piping exposed to flue gas and solutions. Information provided by MetalTek |
Cast Grade CK3MCuN; Cast ASTM A351, A743, A744; Wrought UNS S31254; Wrought Grade 254 SMO® |